| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer
O-Rings, Gaskets and Seals produced from Sanifluor® 1000 have excellent chemical, heat and steam resistance. They provide superior performance in hot water, steam and virtually all caustics; makin..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | UL temperature Index 220/240°C (430/460°F) |
|
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | UL temperature Index 220/240°C (430/460°F) |
|
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | < 50 hours; IEC 60216-P1 |
|
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued **
Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Industrial Laminates/Norplex NP555 Carbon Fiber
(discontinued **)
Description: NP555 is composed of carbon fiber fabric and a phenolic resin system. It has excellent moisture resistance and physical properties. This material was designed to replace asbestos vane m..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | short term |
|
Lehmann & Voss LUVOCOM® 2607-7921 Blend based on polyaryl ether ketone, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Freudenberg Simrit Simriz® 481 Low Temperature FFKT Perfluoroelastomer Compound
Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of ..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Greene Tweed CHEMRAZ® 504 Perfluoroelastomer
Greene Tweeds Chemraz® 504, a 65 Shore A hardness perfluoroelastomer, provides an extremely broad range of chemical resistance and is perfect for services with low pressures and/or low temperatur..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Isoflon Tisoflon® 40S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Isoflon Tisoflon® 6S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Möller Medical NanoSkin 90 NanoCoating
Boiling-water resistant, non-abrasive, dirt-repellant, biocompatible coating with very good chemical resistance.Information provided by Möller Medical, Member of CENTROTEC Group
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Möller Medical PolySkin 95 NanoCoating
Flexible, very non-abrasive, chemical-resistant decorative coating with easy-to-clean propertiesInformation provided by Möller Medical, Member of CENTROTEC Group
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | Heat Resistance; DIN 53772 |
|
Karina 600/167-IE MBPP Blue Color Concentrate
HMF Color Concentrate recommended for polyolefin applications and 2% minimum letdown. This color concentrate meets the FDA regulation.Information provided by Karina Indústria e Comércio de Pl..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Isoflon Tisoflon® 14S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | Short peaks operation |
|
Polyram PlusTek PA840G3 Nylon 6.6, 15% Glass Fiber
15% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | Short peaks operation |
|
Polyram PlusTek PA870G33 Nylon 6.6, 33% Glass Fiber
33% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Trelleborg Emerson & Cuming Eccobond® 104 Two-Component High Temperature Performance Epoxy Adhesive
Emerson & Cuming 104 Eccobond® Two-Component High Temperature Performance Epoxy AdhesiveFilled, heat curing, high temperature resistant, epoxy adhesive. Excellent chemical resistance. Maintains hig..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | Short peaks operation |
|
Polyram PlusTek RA314G50 Nylon 66 for Injection Molding, 50% Glass Fiber Reinforced, Heat Stabilized
50% Glass fiber reinforced, heat stabilized Nylon 66 for injection molding applications.Information provided by Polyram.
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Trelleborg Emerson & Cuming Eccobond® 17 M 1 Heat Cure Catalyst
Emerson & Cuming 17 M 1 Eccobond® Heat Cure CatalystVery high temperature resistance, highest temperature strength, lowest shrink. Non-crystallizing. Long working life. Imparts excellent chemical r..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Trelleborg Emerson & Cuming Stycast® 2762/17M-1 Two-Component Epoxy High Service Temp Encapsulant
Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | Dry Service |
|
Chesterton ARC MXHT High temperature severe wear compound
Description: An advanced ceramic composite for the protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack at elevated temperatures. It is applied at a thickness o..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | short term; EMS |
|
EMS-Grivory Grivory® TSG-30/4 PA666-GF30
Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | short term; EMS |
|
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35
Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Epoxyset Epoxibond EB-348 Low Expansion Epoxy Adhesive
EB-348 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional ..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | DSC |
|
Adamas Adalon® 466 PTFE, Mineral/Organic Filler
Information provided by Adamas, HPM
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | 2 hours |
|
Amity Thermosets ATS 158 Phenolic Molding Glass fiber Filler, Compression Molded
Characteristics:Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications:Switchgear componentCom..
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | |
|
Alliance N-30EZ Neodymium Iron Boron Magnetic Material |
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | Continuous |
|
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer
Fluoropolymer material specifications.Information provided by Isoflon.
|
|||
| Maximum Service Temperature, Air | 230 °C | 446 °F | < 50 hours; IEC 60216-P1 |
|
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed
Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou..
|
|||