| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | Long Term |
|
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer
(discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long time operation |
|
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH
By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads ..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® BGZ-30/2 PA6-GF30
Product description: Grilon BGZ-30/2 is a heat stabilized and impact modified PA6 injection molding grade with 30% glass fibers. Grilon BGZ-30/2 has the following important properties: Good impact s..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40
Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50
Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GV-5H black PA*-GF50
Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50
Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GVS-5H nat PA*-GF50
Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70
Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® L 25H FWA nat PA12
Product Description: Grilamid L 25 H FWA natural is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA natural is designed for technical injection moulded com..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30
Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® LV-15H nat PA12-GF15
Product description: Grilamid LV-15H is a 15% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptiongood dimension..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® LV-23 X ESD PA12-GF23
Product description: Grilamid LV-23 X ESD black is an antistatic Polyamide 12 injection moulding grade with 23 % glass fibre reinforcement. Main attributes are: antistatic with reisitivity < 10^6 O..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30
Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® LV-50H FWA black 9225 PA12-GF50
Product description: Grilamid LV-50H FWA black 9225 is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® LV-5H PA12-GF50
Product description: Grilamid LV-5H is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® TSC-40/4 EC black 9832 PA666-CF40
Information provided by EMS Grivory
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® TSG-30 PA666-GF30
Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30
Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following ..
|
|||
| Maximum Service Temperature, Air | 110 - 120 °C | 230 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® TSGL-40/4 FA black 9840 PA666-GF40
Product description: Grilon TSGL-40/4 FA black 9840 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 FA black 9840 is characterized by th..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® TSK-30/4 PA666-GB30
Product description: Grilon TSK-30/4 is a heat stabilized, normal viscosity PA66 +PA6 injection molding grade with 30% glass beads. Grilon TSK-30/4 has the following important properties: Good surfa..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® TSM-30/2 PA666-MD30
Product description: Grilon TSM-30/2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral filler. Grilon TSM-30/2 has the following important properties: Excell..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® TSM-30/4 PA666-MD30
Information provided by EMS Grivory
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® BGZ-40 PA6-GF40
Product description: Grilon BGZ-40 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 40% glass fibers. Grilon BGZ-40 has the following important properties:..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GV-4H PA*-GF40
Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide...
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50
Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac..
|
|||
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® LBV-30H FWA nat PA12-GF30
Product Description: Grilamid LBV-30H FWA natural is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® BG-50 FC PA6-GF50
Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surfac..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® BRZ 334 H PA6
Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a..
|
|||