| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
|
Nye Lubricants 520M-2-UV (NT) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
|
Nye Lubricants UniFlor 8322 (857A) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
|
Nye Lubricants UniFlor 8921 (892-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
|
Nye Lubricants UniFlor 8981SR (899S-1-RP) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
|
Nye Lubricants UniFlor 8981X (899XP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Precision Polymer Engineering F80R Fluorosilicone Rubber
Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.Applications:
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Precision Polymer Engineering S50G Silicone Rubber
Green Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain.Applications: Excellent heat resistance and low temperature flexibility. Us..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Precision Polymer Engineering S50K Silicone Rubber
Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Federal..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Precision Polymer Engineering S60E Silicone Rubber
Red iron oxide filled, Phenyl Silicone Rubber, 55-65 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Precision Polymer Engineering S60N Silicone Rubber
Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Gr..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Precision Polymer Engineering S70H Silicone Rubber
White Silicone Rubber, 68-78 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States F..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
|
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data)
Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
|
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data)
The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity ..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | Secondary curing mechanism required |
|
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | < 50 hours; IEC 60216-P1 |
|
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7506 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8108 PEEK, with glass fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Improved frict..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8317/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8416 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | short term; EMS |
|
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30
Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
|
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
Product Description: EPO-TEK® 353ND is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. It is one of the most popular EPO-TEK® bra..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | DuPont Test Method |
|
DuPont Performance Polymers Kalrez® Spectrum™ 0090 Fluoroelastomer
DuPont™ Kalrez® 0090 perfluoroelastomer parts deliver durable, reliable sealing solutions for applications requiring excellent rapid gas decompression (RGD) properties as well as high hardness and..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | short term; EMS |
|
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65
Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I..
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | DSC |
|
Adamas Adalon® 406 PTFE, 15% PEEK
Information provided by Adamas, HPM
|
|||
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
|
|||
| Maximum Service Temperature, Air | <= 250 °C | <= 482 °F | Overload protection for brief periods. |
|
Von Roll Isola IMI Irrathene® 201 Irradiated Polyethylene Film
Data provided by Von Roll Isola USA.Produced by electron bombardment of specially formulated polyethylene film used in a wide variety of electrical applications. Irrathene film is nonmelting and hi..
|
|||