| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 130 °C | 266 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL A63 AV15 Nylon 6.6 for injection molding
Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | Electrical |
|
XP Phenolic Laminate
Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Propylene Oxide Rubber (GPO)
Allyl glycidyl ether is a common copolymer with propylene oxide. Good low temperature properties and oxidation/UV resistance but poor oil resistance.
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Lehmann & Voss LUVOCOM® 1850-7854 PBT, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | short term |
|
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK-HB Polycarbonate, with carbon fiber, PTFE, lubricant modified
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Lehmann & Voss LUVOCOM® 50-0789 Polycarbonate, with carbon fiber, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Lehmann & Voss LUVOCOM® 50-7446 Polycarbonate, with carbon fiber, PTFE, lubricant modified
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Lehmann & Voss LUVOCOM® 50-8076 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Industrial Laminates/Norplex NP329 Cotton Fabric
Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, ..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Industrial Laminates/Norplex NP344 Cotton Fabric
Description: Fine weave canvas laminate with high temperature phenolic resin and molybdenum disulfide lubricant. Good machining properties and low coefficient of thermal expansion. Better machining ..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Industrial Laminates/Norplex NP610 Paper Base Laminate
Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/BK PBT, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Industrial Laminates/Norplex NP664 Paper Base Laminate
Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | UL temperature Index, UL 746B |
|
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | UL 746B |
|
Sumitomo Bakelite North America RX® 1-520/RX® 1310 Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, non-flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG.Information provided by Vyncolit, a Sumitomo Bak Group..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | UL temperature Index, UL 746B |
|
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | Continuous use |
|
Polyram RamSter PF310G6 PBT Alloy, 30% Glass Fiber, UV Stabilized
30% Glass fiber reinforced PBT alloy, low warp properties, UV stabilized for injection molding.Information provided by Polyram.
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | Provisional 150, Thermal index; ASTM UL746B |
|
Toyobo VYLOPET® EMC330 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Trelleborg Emerson & Cuming Stycast® 2760 Two-Component Easy Mix Ratio Encapsulant
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, ..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
Cytec (Conap) RN-1210 / EA-028 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
|
|||
| Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | long term; EMS |
|
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60
Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | |
|
3M Scotchcast™ 2123 Re-enterable Insulating Electrical Resin
3M Scotchcast Re-enterable Electrical Resin 2123 is a soft, two-part polybutadine resin encapsulant designed especially for re-enterable splice protection. It is formulated for virtually every elect..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | Emergency Cable |
|
3M Scotch® 13 Electrical Semi-Conducting Tape
Scotch® Electrical Semi-Conducting Tape 13 is a highly conformable, semi-conducting EPR (Ethylene Propylene Rubber) based high-voltage splicing tape. It is non-vulcanizing and shelf stable, with st..
|
|||
| Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | Average value: 140 °C Grade Count:12 |
|
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Maximum Service Temperature, Air | 130 - 250 °C | 266 - 482 °F | Average value: 163 °C Grade Count:8 |
|
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..
|
|||
| Maximum Service Temperature, Air | 130 °C | 266 °F | UL 746B |
|
Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GI..
|
|||