| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
NextGen Adhesives M907-19 Medical Grade Epoxy Adhesive
Description: NGAC M907-19 is a medium viscosity and thixotropic adhesive system that is specifically formulated for medical device assembly applications.Advantages and Applications: Uses include lam..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL B63 H-TF20 Nylon 6 for injection molding, 20% PTFE lubricated
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive
1 to1 mix ratio by volume.TIGA 108 is an epoxy adhesive system that provides excellent bond strength to most substrates. Recommended for production bonding applications, this low viscosity formulati..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
Lehmann & Voss LUVOCOM® 21-8015 Polyamide 6/6T, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
Saint-Gobain Tygon® Norprene® A-60-N Drinking Water Tubing Formulation.
Formulated for use as drinking water tubing. Complies with FDA and NSF61 criteria.Information provided by Saint Gobain Performance Products.
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy
Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable ..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | Continuous; SAE J 2236 |
|
Zylog Neoplast® 187 FT EB Thermoplastic Vulcanizate
Neoplast 187 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
ConocoPhillips Tacna® 2000 NLGI No. 2
Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | Wet Continuous |
|
Chesterton ARC NVE SYSTEM Vinyl Ester Lining
Description: ARC NVE is a high performance, quartz reinforced, three-component, modified novolac vinyl ester lining capable of being applied to horizontal and vertical surfaces. The NVE system kit i..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | Intermittent |
|
Ensinger Tecanat™ Unfilled Polycarbonate (PC)
Tenacat™ is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for ..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | few hours; VDE 0304/P2-1, IEC 216 |
|
EPICHEM Epicarb PC Polycarbonate
Characteristics: high fluidity, good impact
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
|
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned)
Information provided by BASF
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
|
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
|
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
|
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
|
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
|
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
|
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned)
Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
ConocoPhillips SUPER-STA M NLGI No.1
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | 20,000 h; IEC 216/T1 |
|
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail..
|
|||
| Maximum Service Temperature, Air | 135 °C | 275 °F | |
|
LATI Latilon 28D G/30 PC, 30% Glass Fiber Reinforced
Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
|
|||