| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 280 °C | 536 °F | Long Term |
|
Ensinger Sintimid™ V-HPHT high purity high temp Polyimide (PI)
(discontinued **)
SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | < 50 hours; IEC 60216-P1 |
|
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti
Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application ..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-7766 PEEK, with carbon fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-7905 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-7920/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-8160 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-8278/GY PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-8317/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Pigment Heat Resistance; EN 12877-3 |
|
Karina 10/7015-IE White Color Concentrate MBU
Titanium dioxide concentrate, recommended for application in polyolefins and polyolefinic and PVC compounds for general purposes. Recommended usage of 2% to 4%.Information provided by Karina Indú..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-0895/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-7536 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-7914 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Continuous |
|
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | |
|
Dow Corning MOLYKOTE® AS-828 GREASE
Silicone grease with wide service temperature rangeInformation provided by Dow Corning
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Intermittent |
|
Epoxy Technology EPO-TEK® H35-175MPLV Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H35-175MPLV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-el..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Short Periods |
|
Hippe PA 46 Nylon 46
PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Long Term |
|
Brandenburger BL 70 Slide Bearing Material
BL 70 is a low friction material that exhibits stability at high temperatures. Its applications include high-load low friction tracks and linings in transport and conveying systems, high-stressed b..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Long Term |
|
Brandenburger BRA-FLEX Side Insulation
Information provided by Brandenburger Isoliertechnik GmbH&Co.
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Highly Temperature Resistant Quality, Opaque, Grey, Blue |
|
BIW ASTM Class 2D0 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Short term |
|
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Short term |
|
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Short term |
|
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
|
|||
| Maximum Service Temperature, Air | 280 °C | 536 °F | Highly Temperature Resistant Quality, Opaque, Grey, Blue |
|
BIW ASTM Class 2D1 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...
|
|||