| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 300 °C | 572 °F | short period, no load |
|
Omnia Plastica PEEK Polyetheretherketone
Semicrystalline polymer. Material with high mechanical and thermal properties, up to 240°C. It resists to creep under load and to wear, its friction coefficient is low. The temperature resistance w..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | |
|
Premix Thermoplastics PREADD AB 576
PREADD AB 576 is a polypropylene based antiblock masterbatch developed especially for polypropylene cast and blown films.PREADD AB 576 is based on highly purified synthetic silica. Due to its excell..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | |
|
NEXA® PFX8045 Perfluoroelastomer
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | 30% Masterbatch |
|
Premix Thermoplastics PREWHITE PP 22-50
PREWHITE PP 22-50 is a polypropylene based white masterbatch developed for polypropylene extrusion coating applications. Due to the overall balance in the formulation, fast line speeds up to 300 m/m..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Short Term |
|
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC
QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | DIN 53772 |
|
Karina 1000/00851-IE MBPEB White
Mineral concentrated masterbatch, recommended for polyolefins application. Minimum usage from 5%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Heat Resistance; DIN 53772 |
|
Karina 1000/5035-IE MBPEB White Color Concentrate
Masterbatch with 50% of TIO2. Usage from 1% to 5% depending on the client need and necessity of covering.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | DIN 53772 |
|
Karina E 1000/00856-IE MBPEB White
Mineral concentrate, recommended for polyolefinics applications (films/bags). Usage estimated from 10% to 20%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105/XCF/20 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Short Periods |
|
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Short Periods |
|
Dalau Dalcon 086 100% Virgin PTFE modified polymer
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal ..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | |
|
Cymat A35620SC 040SS Stabilized Aluminum Foam
Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it ..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Continuous |
|
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing
Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the ..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | |
|
Destech Open-Celled Glassy Carbon Foam
Destech glassy (vitreous) carbon foam is available in different grades depending on the number of pores per inch (ppi). Standard grades are 10, 45, 100 and 500 ppi. Custom grades are available on a..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Intermittent |
|
Epoxy Technology EPO-TEK® 731 Epoxy Adhesive
Material Description: A two component, thixotropic, room temperature-curing epoxy adhesive. It is an electrically and thermally insulating epoxy designed for general applications in semiconductor p..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Intermittent |
|
Epoxy Technology EPO-TEK® E3037 Epoxy
Material Description: A single component, electrically conductive, thixotropic silver-filled epoxy for die-attach and SMD-attach inside hybrid microelectronics.Information Provided by Epoxy Technolo..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Intermittent |
|
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy
Product Description: EPO TEK® H20E-LC is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also used exte..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Intermittent |
|
Epoxy Technology EPO-TEK® OE138 Two Component Epoxy
Material Description: A two component epoxy with intermediate viscosity range between EPO-TEK® 353ND and EPO-TEK® 353ND-T. It is designed for semiconductor glob top applications, as well as use in..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Intermittent |
|
Epoxy Technology EPO-TEK® H20E Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also ..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | |
|
Abatron AboCast/AboCure 8501-4/8501-4 High Temperature Resistant Epoxy
Gray, high viscosity, structural/machinable epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to be us..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Hot Cutting or Line Bending |
|
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | |
|
BASF Heligoen® Blue L 6905 F Color Additive
Description: Very brilliant a-phthalocyanine blues with high color strength and excellent flocculation resistance (L 6905 F is more brilliant and stronger than L 6901F).Chemical Structure: Cu-phthal..
|
|||
| Maximum Service Temperature, Air | 300 °C | 572 °F | Short term |
|
CENTROPLAST CENTRO HPM Polyetherimide