Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 302 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Recommended
Nye Lubricants 836A (FG) Synthetic Oil
Information provided by Nye Lubricants.
Maximum Service Temperature, Air 150 °C
302 °F
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam
Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti..
Maximum Service Temperature, Air 150 °C
302 °F
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System
Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U..
Maximum Service Temperature, Air 150 °C
302 °F
Cured
Resin Technology Group UV MX-2230 Quick Fixture, Activator Cured, One-Component, Acrylic Adhesive
UV MX 2230 is a one-component acrylate based polymer designed to be used as a quick-fixture, surface activated adhesive, (with optional UV or oven cure), for applications on a variety of substrates ..
Maximum Service Temperature, Air 150 °C
302 °F
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Maximum Service Temperature, Air 150 °C
302 °F
Lehmann & Voss LUVOCOM® 19-8074 Polyamide 46, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
Maximum Service Temperature, Air 150 °C
302 °F
short term
Lehmann & Voss LUVOCOM® 50/CF/7/GS/10/TF/5/EM/BK Polycarbonate, with carbon fiber, glass flakes and PTFE, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Maximum Service Temperature, Air 150 °C
302 °F
short term
Lehmann & Voss LUVOCOM® 50-7228 Polycarbonate, with carbon fiber, glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Maximum Service Temperature, Air 150 °C
302 °F
short term
Lehmann & Voss LUVOCOM® 50-7289/V2 Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Maximum Service Temperature, Air 150 °C
302 °F
Lehmann & Voss LUVOTECH® GS 46 Polyamide 46, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Highly dimensionally stable at e..
Maximum Service Temperature, Air 150 °C
302 °F
short term
Lehmann & Voss LUVOCOM® 50/CF/5/GF/10 Polycarbonate, with carbon fiber and glass fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Maximum Service Temperature, Air 150 °C
302 °F
GrafTech C1 Acrylic Coating
Optional coating for eGRAF® SPREADERSHIELD™ graphite products. Structure: 0.00254mm Acrylic - Graphite
Maximum Service Temperature, Air 150 °C
302 °F
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Maximum Service Temperature, Air 150 °C
302 °F
UL Temperature Index; UL 746B
Sumitomo Bakelite North America RX® 613 Fiberglass Reinforced Phenolic
RXÂ 613 is a fiberglass reinforced phenolic molding compound with good dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North America, Inc.
Maximum Service Temperature, Air 150 °C
302 °F
short term; EMS
EMS-Grivory Grivory® L 16 W 20 black 9995 PA12
Product Description: Grilamid L 16 W 20 is a semi-flexible low viscosity, heat stabilized PA12 injection molding grade. The main characteristics of this product are: Easy flowing?High impact streng..
Maximum Service Temperature, Air 150 °C
302 °F
short term; EMS
EMS-Grivory Grivory® L 20 G grey 9280 PA12
Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low..
Maximum Service Temperature, Air 150 °C
302 °F
short term; EMS
EMS-Grivory Grivory® L 20 H FR PA12 FR
Product Description: Grilamid L 20 H FR is a flame retarded, medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20 H FR contains no halogen or phosphorus, it has a light natural colo..
Maximum Service Temperature, Air 150 °C
302 °F
short term; EMS
EMS-Grivory Grivory® XE 3915 PA12-GF50
Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe..
Maximum Service Temperature, Air 150 °C
302 °F
Continuous use
Daikin NEOFLON RP-5000 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Maximum Service Temperature, Air 150 °C
302 °F
Epoxyset Epoxiohm EO-21 Electrically Conductive Epoxy Adhesive
EO-21 is a two part, silver filled high electrical conductivity epoxy adhesive. It is designed to cure at room temperature or rapidly at elevated temperature and exhibits very excellent adhesion and..
Maximum Service Temperature, Air 150 °C
302 °F
Dow Corning 3-4130 DIELECTRIC GEL KIT
Two-part, clear, heat cure, low extractables.Information provided by Dow Corning
Maximum Service Temperature, Air 150 °C
302 °F
Deflection temperature; load unknown.
Abatron AboCast/AboCure 8109-13
Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45..
Maximum Service Temperature, Air 150 °C
302 °F
Service
3M FM062 Indoor UL Recognized Brite Silver Polyester Label Products
3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
Maximum Service Temperature, Air 150 °C
302 °F
Service
3M FM12B Indoor UL Recognized White Polyester Label Products
3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A..
Maximum Service Temperature, Air 150 °C
302 °F
Service
3M FM165 Indoor UL Recognized Computer Imprintable White Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar..
Maximum Service Temperature, Air 150 °C
302 °F
Service
3M 7025 Screen Printable Polyester Performance Label Products
3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u..
Maximum Service Temperature, Air 150 °C
302 °F
Service
3M 7028FL Screen Printable Polyester Performance LabelProducts
3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st..
Maximum Service Temperature, Air 150 °C
302 °F
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy
Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi..
Maximum Service Temperature, Air 150 °C
302 °F
Chesterton 652 Pneumatic Lubricant & Conditioner
Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e..
Copyright © lookpolymers.com All Rights Reserved