Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
Reltek BONDiT™ B-46 Adhesive, Sealant & Coating System
Key Properties: Excellent adhesion to low surface energy plastics without primer or surface preparation.Applications: Very high flexibility, 500% elongation, emphasizing high tack for un-abraded sub..
Maximum Service Temperature, Air 177 °C
350 °F
Dielectric Polymers NT-5513 High Tack Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati..
Maximum Service Temperature, Air 177 °C
350 °F
Dielectric Polymers NT-2822 Ultra Tack Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out..
Maximum Service Temperature, Air 177 °C
350 °F
Dielectric Polymers NT-702 Acrylic Tape  (discontinued **)
Acrylic adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of non-silicone coated substrates. Provides high temperature s..
Maximum Service Temperature, Air 177 °C
350 °F
Saint-Gobain Rulon® CJ Grade Bearing/Seal PTFE  (discontinued **)
Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of ..
Maximum Service Temperature, Air 177 °C
350 °F
dry
ITW Devcon Metal Repair Titanium Putty, Grey
Information provided by ITW Devcon
Maximum Service Temperature, Air 177 °C
350 °F
dry
ITW Devcon Rubber Repair / Castable Urethane High Temp Edge & Seal (T-36), Amber
Information provided by ITW Devcon
Maximum Service Temperature, Air 177 °C
350 °F
In oxygen
SGL Carbon Group Ridurid® V 1017 High Performance Graphite Filled Plastic
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Maximum Service Temperature, Air 177 °C
350 °F
In oxygen
SGL Carbon Group Ridurid® V 1352 High Performance Graphite Filled Plastic
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Maximum Service Temperature, Air 177 °C
350 °F
Saint-Gobain CHR® 2819-3(R) Acrylic Adhesive Zone Tape
Specification Notes: 21CFR177.1550 compliant. All data based on a 0.003 inch test sample.Information provided by Saint Gobain Performance Products.
Maximum Service Temperature, Air 177 °C
350 °F
Saint-Gobain CHR® 2829-3(R) Acrylic Adhesive Zone Tape
Specification Notes: 21CFR177.1550 compliant. All data based on a 0.003 inch test sample. Information provided by Saint Gobain Performance Products.
Maximum Service Temperature, Air 177 °C
350 °F
Saint-Gobain CHR® M717 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Maximum Service Temperature, Air 177 °C
350 °F
Saint-Gobain CHR® M835 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Maximum Service Temperature, Air 177 °C
350 °F
Saint-Gobain CHR® SG33-05(R) Industrial Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Maximum Service Temperature, Air 177 °C
350 °F
In oxygen
SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Maximum Service Temperature, Air 177 °C
350 °F
Master Bond Supreme 11ANHT Fast Curing Epoxy Paste System
Description: Master Bond Polymer System SUPREME 11ANHT is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevat..
Maximum Service Temperature, Air 177 °C
350 °F
Master Bond Supreme 3HT High Bond Strength One Component Epoxy Adhesive System
Master Bond Polymer System Supreme3HT is a storage stable one component, heat curing epoxy adhesive featuring a hither to unattainable balance of performance properties including both high shear and..
Maximum Service Temperature, Air 177 °C
350 °F
High strength retained
Hexcel® HexWeb® HRP - 1/4 - 4.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Maximum Service Temperature, Air 177 °C
350 °F
High strength retained
Hexcel® HexWeb® HRP - 3/16 - 12.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Maximum Service Temperature, Air 177 °C
350 °F
High strength retained
Hexcel® HexWeb® HRP - 3/8 - 2.2 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Maximum Service Temperature, Air 177 °C
350 °F
High strength retained
Hexcel® HexWeb® HRP - 3/8 - 8.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Maximum Service Temperature, Air 177 °C
350 °F
Hexcel® HexWeb® HRP/F50 - 3.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Maximum Service Temperature, Air 177 °C
350 °F
High strength retained
Hexcel® HexWeb® HRP/OX - 1/4 - 5.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Maximum Service Temperature, Air 177 °C
350 °F
High strength retained
Hexcel® HexWeb® HRP/OX - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Maximum Service Temperature, Air 177 °C
350 °F
Loctite® 3336 Epoxy Light Cure Adhesive
Epoxy Light Cure AdhesivesLoctite® 3336 Epoxy Light Cure AdhesiveA UV cure, medium viscosity two-part epoxy. UV cure effects fast gellation. Complete cure at room temperature or heat cure. Tough an..
Maximum Service Temperature, Air 177 °C
350 °F
Loctite® SpeedBonder™ 325 High Temperature Acrylic Bonding Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
Maximum Service Temperature, Air 177 °C
350 °F
Intermittent
Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6)
VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety ..
Maximum Service Temperature, Air 177 °C
350 °F
Saint-Gobain Rulon® FCJ Grade Bearing/Seal PTFE  (discontinued **)
Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of ..
Maximum Service Temperature, Air 177 °C
350 °F
Dielectric Polymers NT-701 Acrylic Tape  (discontinued **)
Acrylic adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of non-silicone coated substrates. Provides high temperature s..
Copyright © lookpolymers.com All Rights Reserved