| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 149 - 180 °C | 300 - 356 °F | Average value: 161 °C Grade Count:6 |
|
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum..
|
|||
| Maximum Service Temperature, Air | 65.0 - 180 °C | 149 - 356 °F | Average value: 129 °C Grade Count:18 |
|
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
|
|||
| Maximum Service Temperature, Air | 80.0 - 180 °C | 176 - 356 °F | Average value: 126 °C Grade Count:4 |
|
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Maximum Service Temperature, Air | 90.0 - 180 °C | 194 - 356 °F | Average value: 139 °C Grade Count:8 |
|
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
|
|||
| Maximum Service Temperature, Air | 177 - 180 °C | 351 - 356 °F | Softening Range |
|
Huntsman DT 3357 Matting Agent
Color: WhiteComments/Applications: Non-yellowing reactive matting agent for very low gloss epoxy and epoxy/polyester hybrid powder systems. No effect on mechanical properties.Data provided by Ciba ..
|
|||
| Maximum Service Temperature, Air | 170 - 180 °C | 338 - 356 °F | UL 746B |
|
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG-F.Information provided by Vyncolit, a Sumitomo Bak Group
|
|||
| Maximum Service Temperature, Air | 150 - 180 °C | 302 - 356 °F | Continuous |
|
Asahi Glass F-Clean® Film for Greenhouses
F-CLEAN®, produced by Asahi Glass Company, Ltd., is a Ethylene-Tetrafluoroethylene copolymer (ETFE) film used as the preferred covering material for horticultural greenhouses. High ten..
|
|||
| Maximum Service Temperature, Air | 150 - 180 °C | 302 - 356 °F | Continuous |
|
Asahi Glass Fluon® ETFE Film
Applications: Electronics, Energy Saving, Wallpaper, Sound Suppression Walls, Aviation and SpaceInformation provided by Asahi Glass Company, Inc.
|
|||
| Maximum Service Temperature, Air | 90.0 - 180 °C | 194 - 356 °F | Average value: 117 °C Grade Count:6 |
|
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
|
|||
| Maximum Service Temperature, Air | 65.0 - 180 °C | 149 - 356 °F | Average value: 98.9 °C Grade Count:10 |
|
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Maximum Service Temperature, Air | 130 - 180 °C | 266 - 356 °F | Average value: 155 °C Grade Count:7 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
|
|||
| Maximum Service Temperature, Air | 60.0 - 180 °C | 140 - 356 °F | Average value: 131 °C Grade Count:61 |
|
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
|
|||
| Maximum Service Temperature, Air | 160 - 180 °C | 320 - 356 °F | Average value: 166 °C Grade Count:4 |
|
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
|
|||
| Maximum Service Temperature, Air | 65.0 - 180 °C | 149 - 356 °F | Average value: 115 °C Grade Count:5 |
|
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
|
|||
| Maximum Service Temperature, Air | 120 - 180 °C | 248 - 356 °F | Average value: 150 °C Grade Count:15 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
|
|||