| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 190 °C | 374 °F | Intermittent |
|
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled
For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass ..
|
|||
| Maximum Service Temperature, Air | 190 °C | 374 °F | < 50 h; IEC 216/T1 |
|
Raschig Group AMPLA® 7500 melamine-modified polyester
Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta..
|
|||
| Maximum Service Temperature, Air | 190 °C | 374 °F | Short Time; IEC 60216 |
|
PolyOne Bergamid™ B65 G/Mi20 UF grey LS Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Maximum Service Temperature, Air | 190 °C | 374 °F | |
|
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP
BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific..
|
|||
| Maximum Service Temperature, Air | 190 °C | 374 °F | |
|
Menzolit Menzolit® SMC 1500 Unsaturated Polyester UP
SMC 1500 is a special SMC for applications calling for high continuous service temperature. The glass level has been selected to combine good mouldability with good strength and stiffness properties..
|
|||
| Maximum Service Temperature, Air | 190 °C | 374 °F | |
|
Menzolit Menzolit® BMC 3100 Unsaturated Polyester UP
BMC 3100 is a special BMC suitable for the use in head lamp reflectors. Because of its high temperature resistance and dimensional stability as well as low coefficient of thermal expansion, complex ..
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=Error in fixSigDigits: @digits must be between 1 a sec |
374
°F @Time >=Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SGH 5500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Uses: Garden Hose Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time Error in fixSigDigits: @digits must be between 1 a sec |
374
°F @Time Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SGH 5500G Polyvinyl Chloride, Flexible
Availability: Asia Pacific Uses: Garden Hose Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=1800 sec |
374
°F @Time >=0.500 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SGH 6000 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Uses: Garden Hose Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=1800 sec |
374
°F @Time >=0.500 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp DBS 2006 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Ultra High Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=3600 sec |
374
°F @Time >=1.00 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp DBS 8602 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=3600 sec |
374
°F @Time >=1.00 hour |
Congo Red; ASTM D2115-92 |
|
Teknor Apex Sinvicomp SFR 5800C2 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Foamable Uses: Profiles; Foam Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=1800 sec |
374
°F @Time >=0.500 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SFW 4500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Uses: Footwear; General Purpose Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=1800 sec |
374
°F @Time >=0.500 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SIM 5000 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=1800 sec |
374
°F @Time >=0.500 hour |
ASTMD 2115-92 |
|
Teknor Apex Sinvicomp SMG 3500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=1800 sec |
374
°F @Time >=0.500 hour |
ASTMD 2115-92 |
|
Teknor Apex Sinvicomp SMG 5500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=1800 sec |
374
°F @Time >=0.500 hour |
ASTMD 2115-92 |
|
Teknor Apex Sinvicomp SMG 6000 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=Error in fixSigDigits: @digits must be between 1 a sec |
374
°F @Time >=Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SPF 10520 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Uses: Gaskets; Profiles; Seals Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=Error in fixSigDigits: @digits must be between 1 a sec |
374
°F @Time >=Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SPF 4520 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: High Stiffness Uses: Gaskets; Profiles; Seals Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=Error in fixSigDigits: @digits must be between 1 a sec |
374
°F @Time >=Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SPF 7020 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Good Stiffness Uses: Gaskets; Profiles; Seals Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=Error in fixSigDigits: @digits must be between 1 a sec |
374
°F @Time >=Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SPF 9020 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Good Stiffness Uses: Gaskets; Profiles; Seals Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=7200 sec |
374
°F @Time >=2.00 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SRF 2703 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Weather Resistance; Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time 1800 sec |
374
°F @Time 0.500 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SRF 3705 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Medium Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=Error in fixSigDigits: @digits must be between 1 a sec |
374
°F @Time >=Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SRP 4606 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Medium Impact Resistance Uses: Conduit; Piping; Profiles Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=7200 sec |
374
°F @Time >=2.00 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SSH 6009 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Good Flexibility Uses: Cable Jacketing; Wire and Cable Applications Wire Types: ST1; ST2; Type 9; Class 1/3; YM3; YM5 Agency Ratings: BS 6746; IEC 60502; JIS 672..
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=7200 sec |
374
°F @Time >=2.00 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SIH 5008 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Good Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: Y17 Agency Ratings: BS 6746; JIS 6723; VDE 0207 Forms: Pellets Processing Met..
|
|||
| Maximum Service Temperature, Air | 190 °C | 374 °F | Two Hour Heat Resistance per ASTM D648 |
|
Chang Chun Plastic Longlite PM T355J Impact Phenolic Molding Compound
ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd.
|
|||
| Maximum Service Temperature, Air | 190 °C | 374 °F | |
|
Atom Adhesives AA-DUCT 2924 Epoxy Adhesive
AA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage; low resistivity bonding applications where good electrical and physical properties over a wide temperature..
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=Error in fixSigDigits: @digits must be between 1 a sec |
374
°F @Time >=Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp DBS 8615 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air |
190
°C @Time >=3600 sec |
374
°F @Time >=1.00 hour |
Congo Red; BS 2782 |
|
Teknor Apex Sinvicomp SFN 8010 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Oil Resistant Uses: Footwear Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
|
|||