Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 400 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 400 °C
752 °F
Continuous
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite
Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem..
Maximum Service Temperature, Air 400 °C
752 °F
Continuous
Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite
Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to me..
Maximum Service Temperature, Air 400 °C
752 °F
P & P Technology Silver/Aluminum Conductive Adhesive
P & P Technology conductive silver/aluminum adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exp..
Maximum Service Temperature, Air 400 °C
752 °F
Glastic GLASTHERM HT250 Insulation Sheet
Glastherm Grade HT250 is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT250 is asbesto..
Maximum Service Temperature, Air 400 °C
752 °F
GrafTech eGRAF® HITHERM™ HT-705 Graphite
Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat..
Maximum Service Temperature, Air 400 °C
752 °F
GrafTech eGRAF® SPREADERSHIELD™ SS300 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Maximum Service Temperature, Air 400 °C
752 °F
GrafTech eGRAF® SPREADERSHIELD™ SS500 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Maximum Service Temperature, Air 400 °C
752 °F
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Maximum Service Temperature, Air 400 °C
752 °F
oxidation limit
Momentive Performance Materials Pyrolytic Graphite (PG) Coating
PG is a popular coating for sealing machined graphite hardware which does not require oxidation protection. It is the most anisotropic commercially available material and is therefore useful where ..
Maximum Service Temperature, Air 400 °C
752 °F
Goodfellow TZM Molybdenum High Temperature Alloy
Increased high temperature strength over pure molybdenum although, like Molybdenum, it oxidizes rapidly in oxidizing atmospheres above 500°CInformation provided by Goodfellow.
Maximum Service Temperature, Air 400 °C
752 °F
Useful creep to 400°C
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
Maximum Service Temperature, Air 400 °C
752 °F
Eifeler Coatings Technology MoST™ Molybdenum disulfide PVD Coating
MoST™-Molybdenum disulfide as solid lubricant is deposited frequently and successfully as a slide layer on hard coatings.Information provided by Eifeler Coatings Technology
Maximum Service Temperature, Air 400 °C
752 °F
Eifeler Coatings Technology TiCN PVD Coating
Key Characteristics: high hardness excellent abrasive wear resistance, enhanced toughnessPrimary Applications: machining of difficult to machine alloy steels; high performance cutting where moderate..
Maximum Service Temperature, Air 400 °C
752 °F
Eifeler Coatings Technology WC/C PVD Coating
Key Characteristics: high lubricity, low tendency for adhesive wearPrimary Applications: on top of hard coatings for reduction of friction; precision components: automotive, aerospace, medicalInform..
Maximum Service Temperature, Air 400 °C
752 °F
EOS MS1 Maraging Steel for DMLS 3D Printing
EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 100EN Polyimide Film, 25 Micron Thickness
Film thickness 25 micron (1.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 100KN Polyimide Film, 25 Micron Thickness
Film thickness 25 micron (1.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 100ZT Polyimide Film, 25 Micron Thickness
Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 500A Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an ..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 500FPC Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thic..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 500HN Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).Genera..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 500VN Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available ..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 50HN Polyimide Film, 13 Micron Thickness
Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 50KN Polyimide Film, 13 Micron Thickness
Film thickness 13 micron (0.5 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 50ZT Polyimide Film, 13 Micron Thickness
Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 200KN Polyimide Film, 50 Micron Thickness
Film thickness 50 micron 2.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianh..
Maximum Service Temperature, Air 400 °C
752 °F
Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
DuPont™ Kapton® 200ZT Polyimide Film, 50 Micron Thickness
Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available in..
Maximum Service Temperature, Air 400 °C
752 °F
Alloy Wire International RW 45 Ni-Cu Resistance Wire
Used in thermocouples, power resistors, shunts, and wire wound precision restors up to 750°F (400°C)Information provided by Alloywire International.