Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C.
Omnia Plastica PPS GF40 Polyphenylenesulphide
Crystalline polymer based on polyphenylene sulfide with the addition of 40% glass-fibre. Very high rigidity, stiffness and flexural strength. The temperature resistance is very high: up to 240° C. ..
Maximum Service Temperature, Air 230 °C
446 °F
UL temperature Index 220/240°C (430/460°F)
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Maximum Service Temperature, Air 230 - 316 °C
446 - 601 °F
Average value: 263 °C Grade Count:42
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Maximum Service Temperature, Air 230 °C
446 °F
< 50 hours; IEC 60216-P1
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed  (disc
Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area..
Maximum Service Temperature, Air 230 °C
446 °F
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist..
Maximum Service Temperature, Air 230 °C
446 °F
Freudenberg Simrit SC1210 S310 Silicone Elastomer
Excellent material for static service at extreme (hot or cold) temperatures. Outstanding flex and fatigue life. Very good for ozone and UV radiation service as well as for resistance to fungal and b..
Maximum Service Temperature, Air 230 °C
446 °F
Freudenberg Simrit Simriz® 484 FDA FFKT Perfluoroelastomer Compound
Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of ..
Maximum Service Temperature, Air 230 °C
446 °F
Greene Tweed FLUORAZ® 888 Fluoroelastomer, FEPM
Fluoraz® 888 polytetrafluoroethylene/propylene (FEPM) performs well in aggressive chemicals where ultra pure materials are not required. Recommended for conventional wet and dry system applicatio..
Maximum Service Temperature, Air 230 °C
446 °F
Möller Medical NanoSkin 81 NanoCoating
Boiling-water resistant, non-abrasive coating also for plastics with very good chemical resistanceInformation provided by Möller Medical, Member of CENTROTEC Group
Maximum Service Temperature, Air 230 °C
446 °F
Heat Resistance; DIN 53772
Karina 4000/141-IE MBPP Green Color Concentrate
HMF Color Concentrate recommended for polyolefin applications and 2% minimum letdown. This color concentrate meets the FDA regulation.Information provided by Karina Indústria e Comércio de Pl..
Maximum Service Temperature, Air 230 °C
446 °F
Heat Resistance; DIN 53772
Karina 600/167-IE MBPP Blue Color Concentrate
HMF Color Concentrate recommended for polyolefin applications and 2% minimum letdown. This color concentrate meets the FDA regulation.Information provided by Karina Indústria e Comércio de Pl..
Maximum Service Temperature, Air 230 °C
446 °F
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Maximum Service Temperature, Air 230 °C
446 °F
Isoflon Tisoflon® 10S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
Maximum Service Temperature, Air 230 °C
446 °F
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Maximum Service Temperature, Air 230 °C
446 °F
ASTM D1329
Seals Eastern Perflas® 9294 Perfluorinated Rubber
Perfluoro rubber for aggressive chemical service. Perflas ® 9294 seals are made of a chemical resistant perfluorinated fluoroelastomer (FFKM). Perflas 9294 seals offer outstanding resistance to..
Maximum Service Temperature, Air 230 °C
446 °F
Continuous Use
Westlake Plastics Imidex Thermoplastic Polyimide
Made from Aurum® resin. Applications include electronics, acoustics, composites, wire/cable insulation, adhesive film, and washers/gaskets. It will not melt unto itself, is thermoformable, has hi..
Maximum Service Temperature, Air 230 °C
446 °F
Short peaks operation
Polyram PlusTek RA314G50 Nylon 66 for Injection Molding, 50% Glass Fiber Reinforced, Heat Stabilized
50% Glass fiber reinforced, heat stabilized Nylon 66 for injection molding applications.Information provided by Polyram.
Maximum Service Temperature, Air 230 °C
446 °F
short term; EMS
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30
Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi..
Maximum Service Temperature, Air 230 °C
446 °F
short term; EMS
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35
Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Maximum Service Temperature, Air 230 °C
446 °F
short term; EMS
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50
Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Maximum Service Temperature, Air 230 °C
446 °F
short term; EMS
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60
Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Maximum Service Temperature, Air 230 °C
446 °F
Epoxyset Epoxibond EB-115 Unfilled Epoxy Adhesive
A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc...
Maximum Service Temperature, Air 230 °C
446 °F
DSC
Adamas Adalon® 415 PTFE, 10% Organic Filler
Information provided by Adamas, HPM
Maximum Service Temperature, Air 230 °C
446 °F
2 hours
Amity Thermosets ATS 158 Phenolic Molding Glass fiber Filler, Compression Molded
Characteristics:Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications:Switchgear componentCom..
Maximum Service Temperature, Air 230 °C
446 °F
DSC
Adamas Adalon® 451 PTFE, organic filler
Information provided by Adamas, HPM
Maximum Service Temperature, Air 230 °C
446 °F
Alliance N-30EZ Neodymium Iron Boron Magnetic Material
Maximum Service Temperature, Air 230 °C
446 °F
Continuous
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer
Fluoropolymer material specifications.Information provided by Isoflon.
Maximum Service Temperature, Air 230 °C
446 °F
< 50 hours; IEC 60216-P1
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed
Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou..