| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 260 °C | 500 °F | short period, no load |
|
Omnia Plastica PPS GF40 Polyphenylenesulphide
Crystalline polymer based on polyphenylene sulfide with the addition of 40% glass-fibre. Very high rigidity, stiffness and flexural strength. The temperature resistance is very high: up to 240° C. ..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
|
Premix Thermoplastics PREADD SL 502
PREADD SL 502 is a polypropylene based slip masterbatch developed for cast-PP and BOPP films.PREADD SL 502 contains highly purified erucamide, which is neutral in odor and color. PREADD SL 502 does ..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
|
Premix Thermoplastics PREWHITE PE 13-60
PREWHITE PE 13-60 is a PE-LD based white masterbatch, developed especially for medical packages made by injection or blow molding of PE-LD, PE-LLD or PE-HD.Due to the good dispersion PREWHITE PE 13-..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
|
Process Technologies Inc Tyfluor™ 1000 Sanitary Gasket
Tyfluor 1000 is a chemically modified version of PTFE that provides much improved sealing capabilities while maintaining the property characteristics consistent with virgin PTFE material. Tyfluor's ..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | ISO.75 DN.53461 |
|
Polimersan Plastics POLITEF® (PTFE)
POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of ..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | Long Term |
|
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
| Maximum Service Temperature, Air | 260 - 270 °C | 500 - 518 °F | Average value: 263 °C Grade Count:10 |
|
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum ..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-8127 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | short term |
|
Lehmann & Voss LUVOCOM® 1105-8451 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous Service |
|
Solvay Specialty Polymers Algoflon® F 5 Polytetrafluoroethylene (PTFE)
Algoflon® F 5 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for filled grades and in particular is recommended for compounds with glass fiber ..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
|
Saint-Gobain CHR® 2345-2 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
|
Saint-Gobain CHR® SG16-10(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | UL-746 B |
|
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.031" thick)
T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | UL-746 B |
|
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.250" thick)
T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | Short Term (3h) |
|
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous |
|
Trelleborg Sealing Solutions HiMod® 924 Thermoplastic Bearing
Thermoplastic BearingCharacteristics: HiMod® 924 is a high temperature, high modulus material developed for those functions that require high strength and high compressive properties along with exc..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous use |
|
Daikin NEOFLON AP-230ASL PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc...
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous use |
|
Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder
20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | Intermittent |
|
Epoxy Technology EPO-TEK® B9021-6 Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | DSC |
|
Adamas Adalon® 902 PTFE, 1% Conductive filler
Information provided by Adamas, HPM
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
|
Arlon R37053W007 0.007" (0.178 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1 Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 2133 FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneThis data represents ty..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
|
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | DSC |
|
Adamas Adalon® 704 PTFE, Long Carbon Fiber
Information provided by Adamas, HPM
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous |
|
Asahi Glass Fluon® P-63P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous Service |
|
Solvay Specialty Polymers Algoflon® S 121 PTFE (Polytetrafluoroethylene)
(discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
|
|||
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
|
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards
Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and ..
|
|||