| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park AL-2 for Aluminum Solution Heat Treating
A granular mixture of sodium and potassium nitrates formulated per MIL-H-6088. It is less costly than Tempering C-ALHT with only a slight sacrifice in working range. It is colored pink for identif..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park AL-2 Quenching and Tempering Salt
A mixture of nitrates in granular form especially formulated as an economical bath for tempering tool steels requiring treatment within its working range. This highly fluid bath offers low dragout b..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park AL-3 High Speed Hardening Salt
A low-cost granular mixture of nitrates formulated for tempering steels where the lower melting point and wider working range of AL-2 are not needed. Like AL-2, AL-3 is a highly fluid bath that offe..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park Draw Black Cleaning Salt
A salt designed for rapid, thorough and economical cleaning of dies, molds and miscellaneous hardware used in the fabrication of plastics. Also, effective in removing paints, organic binders, oils a..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park High Temp Draw Salt Quenching and Tempering Salt
Salt mixture particularly suitable for ausquenching/austempering. (430 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical.
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park Partherm 430 Heat Transfer Salt
A popular heat transfer salt for use in the higher temperature ranges. It is more inert to ferrous alloys than Partherm 290 or 350 and considerably lower in cost. Its heat capacity and thermal cond..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park Thermo-Quench Quenching and Tempering Salt
Most widely used quench salt for more than a decade. This eutectic nitrate/nitrite mixture is highly recommended for the interrupted or isothermal quenching of austenitized steels. Slightly higher,..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park Parcure 275 Rubber Cure Salt
Nitrate/Nitrite Salt. An eutectic mixture offering the lowest possible melting point and the widest working range. (275 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical.
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park Parcure 305 Rubber Cure Salt
Nitrate/Nitrite Salt. A very popular rubber cure salt that combines wide working range with low cost and relatively lower dragout when used above 400°F. (330 Parkettes)Information provided by He..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park Tempering C-ALHT for Aluminum Solution Heat Treating
A granular mixture of sodium and potassium nitrates formulated per MIL-S-10699-B, class 11 and MIL-H-6088. The salt is colored pink for identification purposesInformation provided by Heatbath Corpo..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | In oxygen |
|
SGL Carbon Group EK 204 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Structural Applications |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Operating Temperature |
|
California Fine Wire Copper, 27% Nickel Clad
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Operating Temperature |
|
California Fine Wire Nickel Alloy 99
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | |
|
Aremco AREMCOLOX™ 502-600 Machinable Glass Ceramic
High dielectric and mechanical strength. For high voltage insulators, lamp housings, thermal switches, and radiation parts. Readily machined, no firing required. Plates from 1/8" to 1" thick; rod..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | |
|
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
|
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | |
|
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone
Low viscosity, green coating for power resistors to 1100°F (593°C)
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | |
|
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
|
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | |
|
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | |
|
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled
Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C).
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | |
|
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating
840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body..
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | |
|
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled
Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C).
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
|
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | |
|
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone
Low viscosity, white coating for motor windings to 1100°F (593°C)
|
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
|
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
|
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
|
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
| Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
|
Heatbath/Park Partherm 290 Heat Transfer Salt
The most widely used heat transfer salt. It is an eutectic mixture with a low melt point and a wide working range. (290 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical.
|
|||