Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 400 °C | 752 °F | |
Glastic GLASTHERM HT250 Insulation Sheet Glastherm Grade HT250 is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT250 is asbesto.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
GrafTech eGRAF® SPREADERSHIELD™ SS1500 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | intercrystalline corrosion resistance, continuous |
H.C. Starck Ampersint® AISI 316 L 300 µm For P/M, HIP/CIP, MIM AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | intercrystalline corrosion resistance, continuous |
H.C. Starck Amperweld® AISI 316 L 150/53 µm for Plasma Transferred Arc Surfacing AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
GrafTech eGRAF® HITHERM™ HT-1210 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
GrafTech eGRAF® HITHERM™ HT-1220 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | oxidation limit |
Momentive Performance Materials Pyrolytic Graphite (PG) Coating PG is a popular coating for sealing machined graphite hardware which does not require oxidation protection. It is the most anisotropic commercially available material and is therefore useful where .. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | intercrystalline corrosion resistance, continuous |
H.C. Starck Ampersint® AISI 316 L 31 µm For P/M, HIP/CIP, MIM AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Good tensile and creep to 400°C |
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Useful creep to 400°C |
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 100EN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 100VN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 200A Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an ar.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 300A Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 300FPC Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 300VN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 500HN Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).Genera.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 500ZT Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available .. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 50FPC Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 50KN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 50ZT Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Intermittent |
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 200HN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General .. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 200VN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available in.. |