Polymer Property : Maximum Service Temperature, Air = 90.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
UL-746 ABC
Plaskolite Optix® CA - 75 UVA General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Maximum Service Temperature, Air 90.0 °C
194 °F
UL 746 ABC
Plaskolite Optix® CA-80 General Purpose Acrylic Resin
Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight.
Maximum Service Temperature, Air 90.0 °C
194 °F
Short Term
Murtfeldt Original Material ”S”® Green Polyethylene
Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen..
Maximum Service Temperature, Air 90.0 °C
194 °F
Short Term
Murtfeldt Original Material ”S”® plus + LF ESD Polyethylene, Low Friction Conductive
This material is electrically conductive and has half the sliding friction coefficient of the Original Material ”S”® enabling voltage to be dissipated at maximum speed with the same maximum frict..
Maximum Service Temperature, Air 90.0 °C
194 °F
Short Term
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction
This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan..
Maximum Service Temperature, Air 90.0 °C
194 °F
UL Temperature Rating
PolyOne Geon™ Vinyl Wire & Cable WELB406L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Maximum Service Temperature, Air 90.0 °C
194 °F
Constant use; SAE J-2236
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous; 20,000 h
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data)
This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie..
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous (GTP 50% Tensile); IEC 60216
PolyOne Bergamid™ A700 BK VN4255 LS Polyamide 66 (Nylon 66)
Information provided by PolyOne
Maximum Service Temperature, Air 90.0 - 160 °C
194 - 320 °F
Average value: 133 °C Grade Count:10
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Maximum Service Temperature, Air 90.0 °C
194 °F
Lehmann & Voss LUVOCOM® 1-7390 Polyamide 66, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Maximum Service Temperature, Air 90.0 °C
194 °F
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el..
Maximum Service Temperature, Air 90.0 - 96.0 °C
194 - 205 °F
Softening point
Mitsui MILEXâ„¢ XL-325M Phenol Aralkyl Resin, High Molecular Weight
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Maximum Service Temperature, Air 90.0 °C
194 °F
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Maximum Service Temperature, Air <= 90.0 °C
<= 194 °F
Sylvin Technologies 6064 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Maximum Service Temperature, Air 90.0 °C
194 °F
Trelleborg Emerson & Cuming Eccobond® 15 LV Clear Variable Hardness Low Viscosity Catalyst
Emerson & Cuming 15 LV Clear Eccobond® Variable Hardness Low Viscosity CatalystLow viscosity. Easy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener ..
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50
Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
EMS-Grivory Grivory® LV-23 ESD PA12-GF23
Product description: Grilamid LV-23 ESD is a 20% fiber reinforced, anti-static injection molding grade Polyamide 12 (PA12). Grilamid LV-23 ESD is heat stabilized, is easy to process and demold. The ..
Maximum Service Temperature, Air 90.0 °C
194 °F
Colorite Polymers CS9040UL Wire and Cable Jacket Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65
Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined..
Maximum Service Temperature, Air 90.0 °C
<br>@Time 7.20e+7 sec
194 °F
<br>@Time 20000 hour
Relative Temperature Index; IEC 216/1
Bond Laminates TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate
Within the TEPEX® composite laminate, PP is a resin known for its good hardness, stiffness, abrasion resistance and chemical resistance.Typical application environments are within automotive applic..
Maximum Service Temperature, Air 90.0 °C
<br>@Time 7.20e+7 sec
194 °F
<br>@Time 20000 hour
Relative Temperature Index; IEC 216/1
Bond Laminates TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea..
Maximum Service Temperature, Air 90.0 °C
<br>@Time 7.20e+7 sec
194 °F
<br>@Time 20000 hour
Relative Temperature Index; IEC 216/1
Bond Laminates TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea..
Maximum Service Temperature, Air 90.0 °C
194 °F
Abatron AboWeld 8709-18/AboCure 50-12 Nickel-Filled Electrically Conductive Epoxy Compound
AboWeld 8709-18/AboCure 50-12 is a practically solventless nickel-epoxy adhesive and resurfacing system with good coating capabilities in the intermediate conductivity range. It is very versatile.
Maximum Service Temperature, Air 90.0 °C
194 °F
3M Scotch™ 2228 Rubber Mastic Tape
3M™ Scotch™ 2228 is a conformable self-fusing rubber electrical insulating sealing tape. Scotch 2228 consist of an ethylene propylene rubber (EPR) backing coated with an aggressive, temperature-st..
Maximum Service Temperature, Air 90.0 °C
194 °F
Trelleborg R721 Natural Rubber Polyisoprene
All information provided by Trelleborg
Maximum Service Temperature, Air 90.0 °C
194 °F
UL-746 ABC
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Maximum Service Temperature, Air 90.0 - 105 °C
194 - 221 °F
Sylvin Technologies 5120 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Maximum Service Temperature, Air 90.0 °C
194 °F
UL Temperature Rating
PolyOne Geon™ Vinyl Wire & Cable W3301 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne