| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
Protective Coating PC-7® Epoxy Paste
PC-7® is a tough job Epoxy formulation developed for maximum bonding power. Components A (grey) and B (black), when mixed, react to form a bond of good strength. PC-7® formulation provides exten..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
Protective Coating PC-SuperEpoxy™ Translucent Epoxy Putty
PC-SUPEREPOXY™ is a non-drip, thixotropic, translucent paste with unlimited uses in bonding, sealing, and as a filler for most materials. Unlike conventional liquid epoxies, PC-SUPEREPOXY™ can be..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
Protective Coating PC-Woody® Epoxy Paste
PC-WOODY® is an epoxy paste formulated to replace missing and rotted wood with structural strength greater than most wood. Use for permanent repairs on all types of wood-exterior or interior. Unl..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
Parker Chomerics CHO-SHIELD® 4900 Conductive Coating
CHO-SHIELD® 4900 silver-filled acrylic coating provides the highest levels of EMI shielding, as well as anti-static protection and grounding surfaces. It offers convenient fast tack and drying. Fil..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
BASF Master Builders Solutions ChemRex® CX-25 Polyurethane Adhesive/Sealant
(discontinued **)
CX-25 is a polyurethane based one-component, moisture curing adhesive/sealant. It provides fast cure, non-sag, excellent adhesion and has elastomeric properties with high strength which can reduce/..
|
|||
| Maximum Service Temperature, Air | <= 93.0 °C | <= 199 °F | continuous use temperature |
|
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 0.6 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of ..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
Henkel Hysol EA 9359.3 Paste Adhesive System
Excellent peel and shear strength. Bonds a variety of substrates.Applications: Structural Repair Composite Bonding
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Dry |
|
Chesterton MRS 5 Metal Rebuilding System
MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
ExxonMobil 325 NC Mobiltac
Mobiltac 375 NC, 325 NC and 275 NC extra high performance non-leaded, diluent-type, heavy-bodied open gear lubricants designed for a wide variety of open gear and mining applications. They contain a..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
3M 2515 Flat Back Paper Masking Tape
3M™ Flat Back Paper Masking Tape 2515 can be used for splicing, bundling, holding, fastening, tabbing and packaging applications.Information provided by 3M
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Long term |
|
3M 3028EK Double Coated Tapes with Adhesive 350
3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a ..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
3M 3900 Multi-Use Duct Tape
3M™ Duct Tape 3900 is a general purpose conformable cloth duct tape made with polyethylene film over cloth scrim and a synthetic rubber adhesive. A good choice for general maintenance, bundling, wr..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Long term |
|
3M 4412G Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
3M 6910 Cloth Gaffers Tape
3M™ Cloth Gaffers Tape 6910 is coated with a rubber adhesive for use in the entertainment industry as “gaffers” tape where light reflection is a concernInformation provided by 3M
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | for 30 mins removes cleanly |
|
3M Scotch® 2480S Ultimate Paint Edge Masking Tape
Scotch® 60 Day Ultimate Paint Edge Masking Tape 2480S uses a thin, yet strong, smooth flat back paper that when used for paint masking gives a sharp paint line with a low paint ridge. This backing ..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Short Term |
|
3M XP2112 Hi-Performance Adhesive Transfer Tape
3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Long Term |
|
3M XT2112 Hi-Tack Adhesive Transfer Tape
3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
3M 4104 Foam Tape
Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
3M 4108 Foam Tape
Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Long term |
|
3M 4411N Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Long term |
|
3M 4412N Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Long term |
|
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Long term |
|
3M 9472FL Adhesive Transfer Tape with 300LSE Adhesive
Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
3M 8979N Performance Plus Duct Tape Nuclear Grade
3M™ Performance Plus Duct Tape 8979N has a unique product construction for indoor and outdoor applications. This tape is removable with little or no adhesive residue from most opaque surfaces up to..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Long term |
|
3M 9593 Double Coated Tapes with Adhesive 350
3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a ..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
3M Scotch® 393 General Purpose Cloth Tape
Scotch® General Purpose Cloth Tape 393 is a polyethylene coated cloth backing coated with a rubber adhesive for moisture-proofing, duct sealing and general purpose applications.Information provided..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
3M 32663 Medium Grey Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | Deflection temperature after post-cure |
|
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge cas..
|
|||
| Maximum Service Temperature, Air | 93.0 °C | 199 °F | |
|
ExxonMobil 325 NC Mobiltac
Mobiltac 375 NC, 325 NC and 275 NC extra high performance non-leaded, diluent-type, heavy-bodied open gear lubricants designed for a wide variety of open gear and mining applications. They contain a..
|
|||