Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 95.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 95.0 °C
203 °F
short period, no load
Omnia Plastica PE 500 - Polyethylene 500
Polyethylene with a molecular weight of ± 500,000. PE 500 is more rigid than the high molecular weight polyethylene and it is therefore more suitable for mechanical applications. The friction coeff..
Maximum Service Temperature, Air 95.0 °C
203 °F
Continuous; 5,000 h
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data)
The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd..
Maximum Service Temperature, Air 95.0 °C
203 °F
Continuous (GTP 50% Tensile); IEC 60216
PolyOne Bergamid™ B650 G/Mi20 UF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Maximum Service Temperature, Air 95.0 - 110 °C
203 - 230 °F
Softening Range
Huntsman HT 3380-1 Special Hardener
Mix Ratio with GT 7013 is 18.Comments/Applications: Acid-anhydride functional crosslinker useful in FDA powder and can coating applications. *Mix ratio with GT 7013.Data provided by Ciba Specialty..
Maximum Service Temperature, Air 95.0 - 105 °C
203 - 221 °F
Softening point
Mitsui MILEXâ„¢ RN-2830MR Acrylic Rubber Modified Phenolic Resin
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Maximum Service Temperature, Air 95.0 - 102 °C
203 - 216 °F
Softening point
Mitsui MILEXâ„¢ RS-2210MB Silicone Rubber Modified Phenolic Resin
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Maximum Service Temperature, Air 95.0 °C
203 °F
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Maximum Service Temperature, Air 95.0 °C
203 °F
Pressed Bushings
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified
Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn..
Maximum Service Temperature, Air 95.0 °C
203 °F
5000 hours; 50% Tensile Strength; IEC 216; DIN 53446
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6)
Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil..
Maximum Service Temperature, Air 95.0 °C
203 °F
Goodfellow Polyhydroxybutyrate - Biopolymer PHB
PHB and its copolymers with polyhydroxyvalerate (PHV) are melt-processable semi-crystalline thermoplastics made by biological fermentation from renewable carbohydrate feedstocks. They have been desc..
Maximum Service Temperature, Air 95.0 °C
203 °F
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Maximum Service Temperature, Air 95.0 °C
203 °F
Zotefoams Plastazote® LD32CN Conductive Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Maximum Service Temperature, Air 95.0 °C
203 °F
Zotefoams Plastazote® MP15FR Metallocene Polyethylene Foam, Flame Retardant
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Maximum Service Temperature, Air 95.0 °C
203 °F
Wet Service
Chesterton ARC 890 Course Grade Sliding Wear Compound
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at the thickness of 6 mm (1/4”)..
Maximum Service Temperature, Air 95.0 °C
203 °F
Wet Service
Chesterton ARC MX1 Vertical Build Extreme Wear Compound
Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It is applied at a thickness of 6 mm (1/4”)..
Maximum Service Temperature, Air 95.0 °C
203 °F
Post Cure, Wet Service
Chesterton MRS S4+ Metal Rebuilding System
An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 ..
Maximum Service Temperature, Air 95.0 °C
203 °F
ASTM D 3575
Eurofoam Porocell POR 304 CM-RS EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Maximum Service Temperature, Air 95.0 °C
203 °F
Wet Service
Chesterton ARC MXC Castable Extreme Wear Compound
Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro..
Maximum Service Temperature, Air 95.0 °C
203 °F
short term; EMS
EMS-Grivory Grivory® TR 90 LXS PAMACM12
Product description: Grilamid TR 90 LXS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LXS natural contains a processing..
Maximum Service Temperature, Air 95.0 °C
203 °F
ASTM D 3575
Eurofoam Porocell POR 304 CM EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Maximum Service Temperature, Air 95.0 °C
203 °F
ASTM D 3575
Eurofoam Porocell POR 304 CM-BI EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Maximum Service Temperature, Air 95.0 °C
203 °F
ASTM D 3575
Eurofoam Porocell POR 304 CM-S EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Maximum Service Temperature, Air 95.0 °C
203 °F
Permanent
3M ScotchCal™ 3690E Graphic Film Material
3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di..
Maximum Service Temperature, Air 95.0 °C
203 °F
Long Term
CENTROPLAST CENTROMID 12 Polyamide 12
This extruded material has good impact resistance, low moisture absorption and good chemical resistance. It is used in precision elements, drive parts, cases and housingsInformation provided by CEN..
Maximum Service Temperature, Air 95.0 °C
203 °F
Zotefoams Plastazote® LD15 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Maximum Service Temperature, Air 95.0 °C
203 °F
short term; EMS
EMS-Grivory Grivory® TR 55 LZ PA12/MACMI
Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LZ offers a variety of interesting properties such as: c..
Maximum Service Temperature, Air 95.0 °C
203 °F
ASTM D 3575
Eurofoam Porocell POR 304 CM-HD 200 EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Maximum Service Temperature, Air 95.0 °C
203 °F
Long Term
CENTROPLAST CENTROMID 6.6 Polyamide 6.6
This material has good hardness, wear resistance, abrasion strength and impact strength. It is used for bearing cages, sliding bearings and articulated joint blocks.Information provided by CENTROPL..
Maximum Service Temperature, Air 95.0 °C
203 °F
Post Cure, Wet Service
Chesterton ARC S4+ 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375..
Copyright © lookpolymers.com All Rights Reserved