| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PP CQX10030E10 F Polypropylene, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PP CQX10030E10 Polypropylene, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPC T1030 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPH TS15010 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPHC T15020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPHC T5040 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPHC T8040 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPC T10030 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPH Q15030 E10 Polypropylene Homopolymer, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 5.00 kg |
291
°F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
|
Cossa Polimeri ESTABLEND 4501 V0/D Flame Retardant PC - ABS
PC - ABS BlendFlame retardant class V0, PBDE and antimony free, with halogens, high impact resistance, very high thermal resistance, high gloss, good processabilityInformation provided by Cossa Poli..
|
|||
| Vicat Softening Point |
144
°C @Load 0.999 kg |
291
°F @Load 2.20 lb |
120°C/hr; ASTM D 1525 |
|
Cossa Polimeri ESTABLEND PSA 7400 HF PC / ASA Blend
Polycarbonate and acrylonitrile styrene acrylate blendHigh impact resistance, high gloss, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
|
|||
| Vicat Softening Point |
144
°C @Load 5.00 kg |
291
°F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
|
Cossa Polimeri ESTACARB 0820 GF Polycarbonate, 10% Glass Filled
Polycarbonate with 10% glass fiber reinforcementHigh stiffness, good impact resistanceInformation provided by Cossa Polimeri S.r.l.
|
|||
| Vicat Softening Point |
144
°C @Load 5.00 kg |
291
°F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
|
Cossa Polimeri ESTACARB 1001 Polycarbonate
General purpose polycarbonateHigh impact resistanceInformation provided by Cossa Polimeri S.r.l.
|
|||
| Vicat Softening Point |
144
°C @Load 5.00 kg |
291
°F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
|
Cossa Polimeri ESTACARB 1601 Polycarbonate
General purpose polycarbonateHigh melt flow rate, high impact resistanceInformation provided by Cossa Polimeri S.r.l.
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
50°C/h; ISO 306 |
|
Covestro Makrolon® 1881 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
120°C/h; ISO 306 |
|
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
120°C/h; ISO 306 |
|
Covestro Makrolon® 2405 MAS056 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
120°C/h; ISO 306 |
|
Covestro Makrolon® 2405 MAS057 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
120°C/h; ISO 306 |
|
Covestro Makrolon® 2407 MAS056 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
50°C/h; ISO 306 |
|
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
120°C/h; ISO 306 |
|
Covestro Makrolon® 2667 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
50°C/h; ISO 306 |
|
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
50°C/h; ISO 306 |
|
Covestro Makrolon® 3107 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
50°C/h; ISO 306 |
|
Covestro Makrolon® FU1007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
|
|||
| Vicat Softening Point |
144
°C @Load 5.10 kg |
291
°F @Load 11.2 lb |
120°C/h; ISO 306 |
|
Covestro Makrolon® LQ2647 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g..
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPH TS15010 H VTUV1 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPHC K8040 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
144
°C @Load 1.00 kg |
291
°F @Load 2.21 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PPHC T8020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||