| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 15.0 W/m-K @Temperature 204 °C |
104 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
| H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
| Thermal Conductivity | 15.0 W/m-K @Temperature 300 °C |
104 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
| Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
| Thermal Conductivity | 15.0 W/m-K @Temperature 23.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
condition H 900 |
| Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
| Thermal Conductivity | 15.0 W/m-K @Temperature 202 °C |
104 BTU-in/hr-ft²-°F @Temperature 396 °F |
|
| Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
| Thermal Conductivity | 15.0 W/m-K @Temperature 23.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
condition H 900 |
| Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
| Thermal Conductivity | 15.0 W/m-K @Temperature 23.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
condition H 900 |
| Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
| Thermal Conductivity | 15.0 W/m-K @Temperature 23.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
condition H 900 |
| Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
| Thermal Conductivity | 15.0 W/m-K @Temperature 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
| Gouda Vuurvast SiC 90 Dense Refractory Brick Description: Very good thermal shock resistance, abrasion resistance as well as very good heat conductivity makes this SiC based brick very well suited for muffles as well as for applications under .. |
|||