Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 160 - 249 °C
7.78 µin/in-°F
<br>@Temperature 320 - 480 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Amodel A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibilit..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 0.000 - 100 °C
7.78 µin/in-°F
<br>@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 150 - 250 °C
7.78 µin/in-°F
<br>@Temperature 302 - 482 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 160 - 249 °C
7.78 µin/in-°F
<br>@Temperature 320 - 480 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 160 - 250 °C
7.78 µin/in-°F
<br>@Temperature 320 - 482 °F
2
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 0.000 - 100 °C
7.78 µin/in-°F
<br>@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 150 - 250 °C
7.78 µin/in-°F
<br>@Temperature 302 - 482 °F
2
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 160 - 250 °C
7.78 µin/in-°F
<br>@Temperature 320 - 482 °F
2
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 0.000 - 100 °C
7.78 µin/in-°F
<br>@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 150 - 250 °C
7.78 µin/in-°F
<br>@Temperature 302 - 482 °F
2
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 150 - 250 °C
7.78 µin/in-°F
<br>@Temperature 302 - 482 °F
2
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
7.78 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM SF2250 PEI Blend (Asia Pacific)
High flow Ultem for thin wall application
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
7.78 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East)
High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
7.78 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM SF2260 PEI Blend (Asia Pacific)
High flow Ultem for thin wall application
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
7.78 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM SF2350 PEI Blend
High flow Ultem blends for thin wall application
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
7.78 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM SF2350 PEI Blend (Asia Pacific)
High flow Ultem blends for thin wall application
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
7.78 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem SF2350 PEI Blend (Europe-Africa-Middle East)
High flow Ultem blends for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
7.78 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DE004 PC
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
7.78 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific)
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
7.78 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DEL22P PC
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Electrically Conductive. Exceptional Processing, Wear..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
7.78 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East)
VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties.
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
7.78 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific)
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
7.78 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM SF2250 PEI Blend
High flow Ultem for thin wall application
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 0.000 - 100 °C
7.78 µin/in-°F
<br>@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0...
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 149 - 249 °C
7.78 µin/in-°F
<br>@Temperature 300 - 480 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 149 - 249 °C
7.78 µin/in-°F
<br>@Temperature 300 - 480 °F
ASTM E831
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..
CTE, linear, Parallel to Flow 14.0 µm/m-°C
<br>@Temperature 150 - 250 °C
7.78 µin/in-°F
<br>@Temperature 302 - 482 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad..
Copyright © lookpolymers.com All Rights Reserved