Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 25.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature >=152 °C
13.9 µin/in-°F

@Temperature >=306 °F
Above Tg; ISO 11359
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific)
PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -20.0 - 150 °C
13.9 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 2200F PEI
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 150 °C
13.9 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2200F PEI
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 150 °C
13.9 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem 2200N PEI
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 150 °C
13.9 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 150 °C
13.9 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 0.000 - 100 °C
13.9 µin/in-°F

@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 150 °C
13.9 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2200 PEI
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 420SE0 PBT
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 420SE0U PBT
PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East)
VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 830F PBT+PET (Asia Pacific)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East)
Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East)
Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
13.9 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
13.9 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature <=143 °C
13.9 µin/in-°F

@Temperature <=289 °F
Below Tg; ISO 11359
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..
Copyright © lookpolymers.com All Rights Reserved