| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific)
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® EFX810ME PC
Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® EFX810ME PC
Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® AD143 PC
LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission ..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® DMX2415 PC
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East)
IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer
High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regi..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML7664 PC Copolymer (Asia Pacific)
Lexan* ML7664 polycarbonate (PC) siloxane resin, is a product targeting (profile) extrusion applications requiring extreme low temperature ductility. Lexan* ML7664 resin is a non-FR product availabl..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® ML7678 PC
17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® PC0700 PC (Europe-Africa-Middle East)
PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® PC1000R PC (Europe-Africa-Middle East)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® PC2200 PC (Asia Pacific)
PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® BFL2000U PC (Europe-Africa-Middle East)
Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics PC0800 PC (Asia Pacific)
PC0800 resin is a low flow (MFR = 8 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics PC1003R PC
PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was ..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics PC1800R PC
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics PC1800R PC (Asia Pacific)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Asia Pacific)
PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL HN731A PPE+PS
PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics PC1800 PC (Asia Pacific)
PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
|
|||
| CTE, linear, Parallel to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||