| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS
PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication.
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific)
PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication.
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according ..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C6200 is a non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. C6200 has improved processing window and edge crac..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS
High flow PC+ABS material designed for local Pacific Automotive applications
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications.
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East)
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East)
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific)
LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific)
7 MFR LEXAN HFD Copolymer
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific)
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Europe-Africa-Middle East)
18 MFR LEXAN High Flow Ductile Copolymer
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer
18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East)
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer
25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Asia Pacific)
High flow PC+ABS material designed for local Pacific Automotive applications
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East)
LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific)
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -30.0 - 80.0 °C |
44.4
µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Europe-Africa-Middle East)
General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA
NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance.
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer
40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Parallel to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific)
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
|
|||