| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
|
SABIC Innovative Plastics Lexan® BFL2015 PC
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® BFL2015 PC
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
|
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
|
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
|
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color.
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color.
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
|
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy
(discontinued **)
Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature 20.0 °C |
22.2
µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide Compound
(Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4-220BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound formulated for enhanced hydrolytic stability in applications requiring ..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature 20.0 °C |
22.2
µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -40.0 - 150 °C |
22.2
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM 4002 PEI
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors.
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature 23.0 - 150 °C |
22.2
µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM 4002 PEI
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors.
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature 0.000 - 100 °C |
22.2
µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-240BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
|
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber
Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
|
Solvay Specialty Polymers Ryton® R-4-280NA Polyphenylene Sulfide (PPS), Glass Fiber
Ryton® R-4-280NA 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
22.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10
LNP* THERMOCOMP* QF0069 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant.
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
22.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6
LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat.
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature 20.0 °C |
22.2
µin/in-°F @Temperature 68.0 °F |
|
|
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C @Temperature 0.000 - 100 °C |
22.2
µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E831 |
|
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..
|
|||