| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific)
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS (Asia Pacific)
PC/ABS with high stiffness and impact performance
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS (Asia Pacific)
PC/ABS with high stiffness and impact performance
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 9945A PC
Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® LSHF PC
Clear PolyCarbonate, High Flow, UV Stabilization, Heat StabilizationThis data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
38.9
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
|
SABIC Innovative Plastics Lexan® LSHF PC (Asia Pacific)
Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Asia Pacific)
High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific ..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer
Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -30.0 - 80.0 °C |
38.9
µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East)
CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature 100 - 200 °C |
38.9
µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
|
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **)
Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East)
Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East)
F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Europe-Africa-Middle East)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East)
Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML6240 PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL FE1630PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1630PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
|
|||