| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific)
Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Asia Pacific)
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer
Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML7647 PC
Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML7647K PC (Asia Pacific)
Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML7666 PC (Asia Pacific)
Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® OQ1022 PC
Standard Flow OQ Resin
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics LNP LUBRILOY D20009P PC
LNP* LUBRILOY* D20009P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant, Exceptional Processing...
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP LUBRILOY D20009P PC
LNP* LUBRILOY* D20009P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant, Exceptional Processing...
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics LNP LUBRILOY D20009P PC (Asia Pacific)
LNP* Lubriloy* D20009P is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant,..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific)
LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics LNP STAT-KON DEI13F PC
LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R..
|
|||
| CTE, linear, Transverse to Flow |
72.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
40.0
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East)
PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the E..
|
|||