| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS
High impact PC+ABS material designed for local Pacific Automotive applications
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific)
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Europe-Africa-Middle East)
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 4404 PPC+PC
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Asia Pacific)
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Asia Pacific)
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific)
7 MFR LEXAN HFD Copolymer
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This ..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 95.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer
Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific)
Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Asia Pacific)
Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer
7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East)
LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific)
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 0.000 - 90.0 °C |
44.4
µin/in-°F @Temperature 32.0 - 194 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East)
VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors.
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Valox® 830F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific)
Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific)
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXRL0681 PC Copolymer
25 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature 100 - 150 °C |
44.4
µin/in-°F @Temperature 212 - 302 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)
(discontinued **)
Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, ..
|
|||
| CTE, linear, Transverse to Flow |
80.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Europe-Africa-Middle East)
25 MFR LEXAN High Flow Ductile Copolymer
|
|||