| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature 23.0 °C |
30.6
µin/in-°F @Temperature 73.4 °F |
ASTM D696 |
|
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature 200 °C |
30.6
µin/in-°F @Temperature 392 °F |
ASTM D696 |
|
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 150 °C |
30.6
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Ultem 1010A PEI (Europe-Africa-Middle East)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 150 °C |
30.6
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Ultem 1100EF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature 23.0 - 150 °C |
30.6
µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Ultem 1100EF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 150 °C |
30.6
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 150 °C |
30.6
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Ultem 1110V PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 150 °C |
30.6
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM 9011 PEI
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion.
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 150 °C |
30.6
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM 9011 PEI (Europe-Africa-Middle East)
Transparent, high flow Polyetherimide (Tg 217C). Resin is RoHS compliant. Improved processability for Fiber extrusion.
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature 0.000 - 100 °C |
30.6
µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -20.0 - 150 °C |
30.6
µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Ultem DH1004F PEI (Asia Pacific)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific ..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -20.0 - 150 °C |
30.6
µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Ultem DH1004F PEI (Europe-Africa-Middle East)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature 23.0 - 150 °C |
30.6
µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 150 °C |
30.6
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM HU1000E PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature 23.0 - 150 °C |
30.6
µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 150 °C |
30.6
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific)
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -20.0 - 150 °C |
30.6
µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM 9090 PEI
Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution.
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -50.0 - 50.0 °C |
30.6
µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber
Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta..
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature -40.0 - 150 °C |
30.6
µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East)
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
|
|||
| CTE, linear, Transverse to Flow |
55.0
µm/m-°C @Temperature 23.0 - 150 °C |
30.6
µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East)
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
|
|||