Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 70.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Asia Pacific)
High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics.
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Europe-Africa-Middle East)
High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics.This data was supplied by SABIC-IP for the Europe..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® 505R PC
Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm...
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. ..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 95.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 95.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FXM123R PC (Asia Pacific)
FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package ..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® HFD4413 PC
Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® HPS1S PC
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific)
Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® ML6413 PC
Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer
Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific)
Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regio..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics Lexan® BFL2000U PC
Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature 100 - 200 °C
38.9 µin/in-°F
<br>@Temperature 212 - 392 °F
ISO 11359-2
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin &nbsp;(discontinued **)
Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region.