| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East)
Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications.
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS
Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS (Asia Pacific)
Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS
Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1...
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Asia Pacific)
Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1...
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1...
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East)
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer
Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® HPS7R PC
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East)
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Asia Pacific)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® HPS7 PC
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific)
PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications.
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East)
VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets.
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific)
Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications.
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East)
Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts..
|
|||
| CTE, linear, Transverse to Flow |
75.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC
LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated.
|
|||