| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycolac® MG8000SR ABS
This data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Cycolac® MG94U ABS
High flow, UV stabilized ABS molding grade
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 505RU PC
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific)
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East)
Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 23.0 - 150 °C |
47.2
µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® 4012G PBT
VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 100 - 200 °C |
47.2
µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 100 - 200 °C |
47.2
µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 100 - 200 °C |
47.2
µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® XE4050BL Polyphenylene Sulfide Alloy (PPS Alloy), GlassMineral Filled
Ryton® XE4050BL glass fiber and mineral filled polyphenylene sulfide alloy compound provides high ductility and impact strength along with good thermal stability.Features: Ductile; Good Thermal S..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
47.2
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® 815F PBT+PET
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East)
XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA
NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Europe-Africa-Middle East)
NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance.
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 60.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 60.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 100 - 200 °C |
47.2
µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
|
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Asia Pacific)
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
|
|||
| CTE, linear, Transverse to Flow |
85.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
|
|||