Polymer Property : Specific Heat Capacity = 2.25 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F127 PA6
Low/Medium Viscosity, Film Extrusion
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F130 PA6
Film Extrusion, Medium Viscosity
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F130-E1 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F130-E5 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F132-E1 PA6
Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F132-E2 PA6
High Viscosity, Nucleated, Lubricated, Film Extrusion
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F136 PA6
Very High Viscosity, Film Extrusion
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F136-C PA6
Film Extrusion, Very High Viscosity, Lubricated
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F136-C1 PA6
Very High Viscosity, Film Extrusion, Lubricated
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F136-E1 PA6
Very High Viscosity, Lubricated, Nucleated, Film Extrusion
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F136-E2 PA6
Very High Viscosity, Lubricated, Nucleated, Film Extrusion
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® XP36-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® F128 PA6
Film Extrusion, Medium Viscosity
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® XP32-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Specific Heat Capacity 2.25 J/g-°C

@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F

@Temperature 68.0 - 302 °F
DSM Akulon® XP36-E1 PA6
Film Extrusion, Medium Viscosity, Nucleated, Lubricated