| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 180 - 200 °C | 356 - 392 °F | Resin temp |
|
Asahi Kasei Tenac®-C 8554 Acetal Copolymer, High Flow
(discontinued **)
Superhigh-flow grade, with properties necessary for VCR reels.Applications: VCR reels.This product is not a part of the standard product line dated 2003.
|
|||
| Processing Temperature | 190 - 200 °C | 374 - 392 °F | Mixture Zone |
|
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend
The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along ..
|
|||
| Processing Temperature | 170 - 200 °C | 338 - 392 °F | |
|
IRPC Polimaxx Polene G2855 High Density Polyethylene
CHARACTERISTICS:GOOD IMPACT STRENGTH, MEDUIM STIFFNESSGOOD PROCESSABILITYAPPLICATIONS:BLOW MOLDINGFOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES,COSMETIC BOTTLES, CHEMICAL CONTAI..
|
|||
| Processing Temperature | 150 - 200 °C | 302 - 392 °F | |
|
Kraton® D1116 (SB)n Branched Copolymer
(SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve ..
|
|||
| Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
|
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet
High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines..
|
|||
| Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
|
KYDEX® V Acrylic/PC Thermoplastic Sheet
Utility sheetApplications: Can be used to substitute effectively for utility grade thermoplastics. It is very appropriate for hidden parts and painted parts and/or where fire retardancy is not requ..
|
|||
| Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
|
Lucobit Lucofin® 1412-t2 Polyolefin TPO Granules, Light Grey
Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t2 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and ..
|
|||
| Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
|
Lucobit Lucofin® 1413-t3 Polyolefin TPO Granules, Dark Grey
Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t3 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and ..
|
|||
| Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
|
KYDEX® 6185 Thermoplastic Sheet
High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar..
|
|||
| Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
|
KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet
Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest sh..
|
|||
| Processing Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Taiwan Sheen Soon Sheenthane® A7530 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
|
|||
| Processing Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Taiwan Sheen Soon Sheenthane® A8530 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
|
|||
| Processing Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Taiwan Sheen Soon Sheenthane® A8550 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD.
|
|||
| Processing Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Taiwan Sheen Soon Sheenthane® A8556K Film Grade Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD.
|
|||
| Processing Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Taiwan Sheen Soon Sheenthane® A8630F Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
|
|||
| Processing Temperature | 120 - 200 °C | 248 - 392 °F | |
|
Fainplast Compounds Hax™ HFX 500S Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing for solar cablesInformation provided by Fainplas..
|
|||
| Processing Temperature | 120 - 200 °C | 248 - 392 °F | |
|
Fainplast Compounds Hax™ HFX 509 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla..
|
|||
| Processing Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Wanhua Chemical Wanthane® WHT-2180 Polycaprolactone Based TPU
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
|
|||