| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 284 °C Grade Count:25 |
|
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 284 °C Grade Count:5 |
|
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
|
|||
| Processing Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Honeywell Aegis™ CSD High Barrier Nylon
(discontinued **)
Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss LUVOCOM® 3/CF/30/EG Polyamide 6, with carbon fiber, extrusion grade
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss LUVOCOM® 55-7880 PC/ABS Alloy, with carbon fiber and glass fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me..
|
|||
| Processing Temperature | <= 270 °C | <= 518 °F | |
|
Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesHigh heat resistanceChemical resistance, hydrolysis resistanceGood paint adhesionHigh flow ability,..
|
|||
| Processing Temperature | <= 270 °C | <= 518 °F | |
|
Kingfa UTPBT-HB Toughened PBT
Features:High impactExcellent size stabilityEasy processingApplications:Injection moldingSwitch partsKeyboard keysE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Processing Temperature | 270 °C | 518 °F | |
|
Tipco Tipcofil® KMX 800 FR - UL94-V0 Flame Retardant, Highly Filled PBT/PC Alloy, with High Heat Stability
Highly Filled, Flame Retardant PBT/PC Alloy, for Injection Molding of "Ceramic Effect" PartsApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacture..
|
|||
| Processing Temperature | 270 °C | 518 °F | Extruder Temperature |
|
DSM Akulon® F127 PA6
Low/Medium Viscosity, Film Extrusion
|
|||
| Processing Temperature | 270 °C | 518 °F | Extruder Temperature |
|
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
|
|||
| Processing Temperature | 270 °C | 518 °F | Extruder Temperature |
|
DSM Akulon® F136 PA6
Very High Viscosity, Film Extrusion
|
|||
| Processing Temperature | 270 °C | 518 °F | Extruder Temperature |
|
DSM Akulon® F136-C1 PA6
Very High Viscosity, Film Extrusion, Lubricated
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR25 NL HS PA6.6, 25% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR40 NL RM PA6.6, 40% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
|
Eurotec® Tecopet® PT70 GR20 NL100 PR PET, 20% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
|
Eurotec® Tecopet® PT70 GR30 NL100 HT PET, 30% glass fiber reinforced, high heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
|
E-Polymers TEKANATE™ G730 , 30% Glass Fiber Reinforced Poly Carbonate
30% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 KC50 BK111 PA6.6, 50% glass/carbon fiber reinforced, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
|
Eurotec® Tecomid® NA40 NL E PA6.6, unfilled, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
|
Eurotec® Tecopet® PT70 GR30 NL100 PR PET, 30% glass fiber reinforced, high heat stabilized, natural, fast crystallization grade
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
|
Eurotec® Tecotek® PC40 GR20 NL PC, 20% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
|
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
|
Arkema Group LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4503 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process.LOTADER 4503 is a versatile adhesive for extrusion lamination, des..
|
|||