| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 275 °C | 527 °F | |
|
Nylene® 734 Nylon 6
Dry as molded. Injection molding grade. Nylene 734 is the heat stabilized version of 733 which is a high impact modified nylon suitable for both molding and extrusion. In addition to heat stabiliza..
|
|||
| Processing Temperature | 275 °C | 527 °F | |
|
Nylene® NX3055I Nylon 6
Dry as molded. Film Grade. Nylene NX3055I is an extrusion grade nylon 6 suitable for cast film, blown film, and co-extrusion applications. NX3055I is highly crystalline which yields excellent roll..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with..
|
|||
| Processing Temperature | 275 °C | 527 °F | Extruder forward zone and adapter. |
|
DuPont Bynel® 2014 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **)
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
|
|||
| Processing Temperature | 275 °C | 527 °F | Extruder forward zone and adapter. |
|
DuPont Bynel® E403 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **)
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
|
|||
| Processing Temperature | 275 °C | 527 °F | Typical extrusion metering zone. May be extruded up to 300°C. |
|
DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin
(discontinued **)
Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and perfor..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and perfor..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista..
|
|||
| Processing Temperature | 275 - 295 °C | 527 - 563 °F | |
|
Ter Hell Plastic Terez® PA 6.6 HT 7110 GF 41 FL-HF/2 Polyamide 66 Copolymer, 41% Glass Fiber
Description: Partly aromatic Polyamide 6.6 Copolymer, 41% glass fiber reinforced and flame retardants.Application:Stiff molding parts with high stiffness by outstanding thermal stability, reduced w..
|
|||
| Processing Temperature | 275 - 315 °C | 527 - 599 °F | |
|
Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon
D870 = Transparent Amorphous Nylon for Injection Molding, Unlubricated. D870L = Transparent Amorphous Nylon for Injection Molding, Lubricated.Data provided by the manufacturer
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is ..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined ..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8331G HS Blend Impact Modified, 14% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8331G HS Blend is a 14% glass fiber reinforced, heat stabilized, polyamide 6 molding compound developed for applications requiring improved toughness in combination with a balance of strength..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8332G Impact Modified, 25% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8332G is a 25% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of ..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance ..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8351 HS BK-102 Impact Modified Nylon 6 (Dry)
(discontinued **)
Capron 8351 HS BK-102 is a heat stabilized, pigmented black type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughness combined with a moderate fle..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® 8362 HS BK-102 Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8362 HS BK-102 is a pigmented black, 34% mineral reinforced, impact modified, heat stabilized nylon 6 injection molding compound exhibiting a high level toughness in combination with excellen..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® HPN 9315G Impact Modified, 15% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron HPN 9315G is a 15% glass reinforced, impact modified polyamide 6 injection molding grade resin in the High Productivity Nylon Series developed for applications requiring superior dry-as-molde..
|
|||
| Processing Temperature | 275 °C | 527 °F | See Materials Notes |
|
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with..
|
|||