| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 284 °C Grade Count:25 |
|
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 285 °C Grade Count:38 |
|
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 289 °C Grade Count:31 |
|
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
|
|||
| Processing Temperature | 80.0 - 300 °C | 176 - 572 °F | Average value: 277 °C Grade Count:21 |
|
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Ter Hell Plastic Terez® PC X 9005 GF 5 Polycarbonate, 5% Glass Fiber
Description: Polycarbonate, medium flowability, 5% glass fiber reinforced.Application: For injection molded parts with increased demand of stiffness.Information provided by Ter Hell Plastic GMBH.
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GB30 NL HS PA6.6, 30% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR15 NL HS PA6.6, 15% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR25 NL HS PA6.6, 25% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR40 NL HS PA6.6, 40% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 MF40 BK001 HS PA6.6, 40% mineral filled, heat stabilized, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET
40% GF/MF Reinforced, Low warpageInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 AR20 NL HS PA6.6, 20% aramid fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 CR10 BK111 PA6.6, 10% carbon fiber reinforced, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 CR30 BK111 PA6.6, 30% carbon fiber reinforced, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NAX0 GR70 NL HS PA6.6, 70% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 260 - 300 °C | 500 - 572 °F | |
|
Eurotec® Tecotek® PC30 NL RX PC, unfilled, improved flow & low temperature impact, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET
45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 240 - 300 °C | 464 - 572 °F | Injection |
|
Arkema Group Rilsan® Clear G380 Renew Polyamide
Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited..
|
|||
| Processing Temperature | 240 - 300 °C | 464 - 572 °F | Resin Temperature |
|
Asahi Kasei Xyron® 640Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
|
|||
| Processing Temperature | 280 - 300 °C | 536 - 572 °F | Resin Temperature |
|
Asahi Kasei Xyron® A0210 PPE/PA
AutomotiveInformation provided by Asahi Kasei
|
|||
| Processing Temperature | 285 - 300 °C | 545 - 572 °F | Melt |
|
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM
Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering ..
|
|||
| Processing Temperature | 170 - 300 °C | 338 - 572 °F | |
|
Asahi Kasei ASACLEAN HP Polypropylene Based Purging Compound
HP was developed for Polypropylene color changes for large parts and hot runner cleaning. Its higher melt flow makes HP Grade suitable for high cavitation hot runner cleaning. HP Grade is moldable a..
|
|||
| Processing Temperature | 110 - 300 °C | 230 - 572 °F | Average value: 237 °C Grade Count:5 |
|
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
|
|||
| Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
|
E-Polymers TEKAMID® TA210G15 , 15% Glass Fiber Reinforced PA66, DAM
Beautiful surface, strength propertyInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
E-Polymers TEKAMID® TB120GM40 , 40% GF/MF Reinforced PA6, DAM
40% GF/MF reinforced, Good surface, Low warpageInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 285 - 300 °C | 545 - 572 °F | Melt |
|
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded
Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo..
|
|||