| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 182 - 204 °C | 360 - 399 °F | Optimum Extrusion Conditions |
|
DSM Biomedical PurSil® 10 Thermoplastic Silicone Polyether Urethane
(discontinued **)
PurSil® thermoplastic siliconepolyether-urethane (TSPU) is a novel copolymer that is strong, yet flexible with proven biocompatibility and biostability. Leveraging the benefits of both silicone ela..
|
|||
| Processing Temperature | 182 - 204 °C | 360 - 399 °F | |
|
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **)
PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether..
|
|||
| Processing Temperature | 182 - 204 °C | 360 - 399 °F | |
|
DSM Biomedical PurSil® AL 20 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **)
PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether..
|
|||
| Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
|
Chevron Phillips Marlex® HHM 5502-02 LW High Density Ethylene Hexene Copolymer
(discontinued **)
High Density Ethylene Hexene Copolymer with Synthetic AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and mos..
|
|||
| Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
|
Chevron Phillips Marlex® HHM 5502-02 LD High Density Ethylene Hexene Copolymer with Antistat
(discontinued **
High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergen..
|
|||
| Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding Stock |
|
Chevron Phillips Marlex® HHM 5502-04BN HDPE Hexene Copolymer
(discontinued **)
This resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergents. Meets ASTM D4976 - PE 235. ASTM D1248 - Type III, Class A, Cat..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | Average value: 163 °C Grade Count:12 |
|
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 462 Ethylene-Vinyl Acetate Copolymer Resin
(discontinued **)
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 163 - 204 °C | 325 - 399 °F | Thermoforming |
|
KYDEX® 430 ABS/PVC Blend for Medical Device Housings
KYDEX® 430 is an ABS/PVC thermoplastic sheet that offers superior thermoformability, rigidity, breakage resistance, chemical resistance and fire retardancy.Features:Good for deep or hard to form ..
|
|||
| Processing Temperature | 160 - 204 °C | 320 - 399 °F | Injection |
|
Dyna-Purge® V Purging Compound
Designed for Purging Flexible and Rigid PVCGeneral Description:DYNA-PURGE V is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow naturally throug..
|
|||
| Processing Temperature | 160 - 204 °C | 320 - 399 °F | Extrusion |
|
Dyna-Purge® V Purging Compound
Designed for Purging Flexible and Rigid PVCGeneral Description:DYNA-PURGE V is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow naturally throug..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 265 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 360 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 750 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
|
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of products. Has exce..
|
|||
| Processing Temperature | 182 - 204 °C | 360 - 399 °F | Optimum Extrusion Conditions |
|
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU)
A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional..
|
|||
| Processing Temperature | 93.0 - 204 °C | 199 - 399 °F | |
|
DuPont Teijin Films Mylar® 854 Polyester Packaging Film, 60 Gauge
Data provided by DuPont Packaging Polymers.DuPont Melinex® DuPont Melinex® 854 is a clear, one side coextruded heat sealable surface similar to Melinex® 850. The opposite surface is adhesion pret..
|
|||
| Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
|
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers ..
|
|||
| Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
|
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers ..
|
|||
| Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
|
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat
High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of product..
|
|||
| Processing Temperature | 182 - 204 °C | 360 - 399 °F | Optimum Extrusion Conditions |
|
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU)
A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional..
|
|||
| Processing Temperature | 182 - 204 °C | 360 - 399 °F | Average value: 193 °C Grade Count:5 |
|
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..
|
|||
| Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
|
DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||