| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber
(discontinued **)
A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 253-36 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 253-50 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 451-87 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 453-45 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
ExxonMobil Santoprene® 8211-45W237 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
ExxonMobil Santoprene® 151-60 Thermoplastic Rubber
(discontinued **)
Description: A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. ..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
ExxonMobil Santoprene® 121-80M300 Thermoplastic Rubber
(discontinued **)
Description: A black thermoplastic high-flow elastomer for excellent injection molding performance with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloropren..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber
(discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 8281-55 Thermoplastic Rubber
(discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber
(discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
(discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
ExxonMobil Vyram™ 9271-65 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
ExxonMobil Vyram™ 9271-85 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | Optimum Tunnel temperature range. |
|
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
|
|||
| Processing Temperature | 215 - 232 °C | 419 - 450 °F | Preheat |
|
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
|
|||
| Processing Temperature | 20.0 - 232 °C | 68.0 - 450 °F | Average value: 180 °C Grade Count:11 |
|
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
|
|||
| Processing Temperature | 221 - 232 °C | 430 - 450 °F | Soldering Range |
|
Lucas-Milhaupt Silvabrite® Lead-Free Solder
Silvabrite silver/tin soldering alloys have been engineered specifically for field repair. These silver/tin solders have been specifically formulated to make difficult repairs swiftly and confidentl..
|
|||
| Processing Temperature | 188 - 232 °C | 370 - 450 °F | Blow Molding |
|
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer
Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55..
|
|||
| Processing Temperature | 193 - 232 °C | 379 - 450 °F | Extrusion |
|
Chevron Phillips Marlex® K606 High Density Polyethylene
High Density PolyethyleneCustomer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.Applications: Recommended resin for thin sheet, cut sheet up to..
|
|||
| Processing Temperature | 192 - 232 °C | 378 - 450 °F | Stock temperature depending on base resin used |
|
Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate
Characteristics: excellent thermal stability, a long useful outdoor life, good processabilityApplications: geomembranes, sheets and thermoforming, blow moldingProcessing: 192-232°C stock temperatur..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 251-85 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
|
|||
| Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
|
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
|
|||
| Processing Temperature | 216 - 232 °C | 420 - 450 °F | |
|
Westlake Mxsten CV77526 Polyethylene Plastomer
Mxsten CV Plastomer CV77526 resin is a polyethylene plastomer designed for blown film extrusion and food packaging that contains no slip and no antiblock additives. Films produced with this resin ex..
|
|||