| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | <= 260 °C | <= 500 °F | |
|
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra..
|
|||
| Processing Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
|
|||
| Processing Temperature | 260 °C | 500 °F | See Materials Notes |
|
BASF Capron® 1202CQ Nylon 6 (Dry)
(discontinued **)
Capron 1202CQ is a blended low viscosity, polyamide 6 injection molding homopolymer, possessing a modified crystalline structure for increased property performance and faster cycles. It is also ava..
|
|||
| Processing Temperature | 260 °C | 500 °F | |
|
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Air Intake Module
SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using..
|
|||
| Processing Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Eastman Tritan MX711 Copolyester
Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co..
|
|||
| Processing Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Eastman Tritan TX2000 Copolyester
Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc..
|
|||
| Processing Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Eastman Tritan TX2001 Copolyester
Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe..
|
|||
| Processing Temperature | <= 260 °C | <= 500 °F | |
|
DuPont™ Bynel® 41E850 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
|
|||
| Processing Temperature | <= 260 °C | <= 500 °F | |
|
DuPont™ Surlyn® E185SB Ionomer Resin
Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed..
|
|||
| Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
|
E-Polymers TEKAMID® TB120G15T Impact Modified, 15% Glass Fiber Reinforced PA6, DAM
15% GF reinforced, Good impact resistanceInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade
Information provided by Eurotec®
|
|||
| Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Eurotec® Tecopet® PT74 GR30 NL XA60 PET, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free,, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | <= 260 °C | <= 500 °F | |
|
Addcomp ADD-VANCE® FR 825 EVA based flame-retardant masterbatch
Fields of application: Injection- or compression molded articles and extruded parts.Examples: Foils, films, tapes and ropes, crates, electronic equipment and other extruded/injection molded articles..
|
|||
| Processing Temperature | 260 °C | 500 °F | Fast cure is 10 min. @ 500°F |
|
Armstrong A-706 Epoxy Adhesive
A one-component, gray, aluminum-filled, thixotropic, non-sag epoxy adhesive. A-706 has an in-service temperature range to 400°F, but requires 350°F minimum cure temperature. Features excellent m..
|
|||
| Processing Temperature | 260 - 300 °C | 500 - 572 °F | Resin Temperature |
|
Asahi Kasei Xyron® X5402 PPE/PA
Oil ResistantInformation provided by Asahi Kasei
|
|||
| Processing Temperature | 260 °C | 500 °F | Cure 30 sec; through solder reflow process |
|
Aptek 2313-PMF Hybrid Epoxy Adhesive
Snap-cure, silver-filled; long pot-life/stable viscosity-excellent for robotics. Thermal shock resistant.Production-oriented, snap-cure technology for surface mount applications-allows cure during s..
|
|||
| Processing Temperature | 260 °C | 500 °F | See Materials Notes |
|
BASF Capron® 8202C HS Nylon 6 (Dry)
(discontinued **)
Capron 8202C HS is a heat stabilized, low viscosity, polyamide 6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It i..
|
|||
| Processing Temperature | <= 260 °C | <= 500 °F | |
|
DuPont™ Fusabond® M603 Polymer Modifier
Fusabond® M603 Resin is a random ethylene copolymer, incorporating a monomer which is classified as being a maleic anhydride equivalent for application uses.Fusabond® M603 is used in a variety of ..
|
|||
| Processing Temperature | <= 260 °C | <= 500 °F | |
|
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties..
|
|||
| Processing Temperature | <= 260 °C | <= 500 °F | |
|
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen..
|
|||
| Processing Temperature | 260 - 280 °C | 500 - 536 °F | Resin Temperature |
|
Asahi Kasei Xyron® A0100 PPE/PA
AutomotiveInformation provided by Asahi Kasei
|
|||
| Processing Temperature | 260 - 285 °C | 500 - 545 °F | Average value: 280 °C Grade Count:5 |
|
Overview of materials for Ionomer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
|
|||