| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 280 °C | 518 - 536 °F | Average value: 275 °C Grade Count:4 |
|
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss LUVOCOM® 3/TF/20/BK Polyamide 6, with PTFE
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss LUVOCOM® 3-7451 Polyamide 6, lubricant modified, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Processing Temperature | 270 °C | 518 °F | mass temp |
|
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG
|
|||
| Processing Temperature | 270 °C | 518 °F | Molding temperature |
|
Toyobo VYLOPET® CA5310 PC/PBT Polymer Alloy, High Rigidity, Impact Resistant
Applications: Lamp partsHome electric appliance partsFeatures: Fine appearanceHigh rigidityImpact resistantInformation provided by Toyobo.
|
|||
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
|
Ter Hell Plastic Terez® PA 6.6 7510 GF 50 Polyamide 66, 50% Glass Fiber
Description: PA66 with medium viscosity, 50% glass fiber reinforced.Application: For molding parts with very high stiffness at good thermal stability.Information provided by Ter Hell Plastic GMBH...
|
|||
| Processing Temperature | 270 °C | 518 °F | Extruder Temperature |
|
DSM Akulon® F130-E5 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock
|
|||
| Processing Temperature | 270 °C | 518 °F | Extruder Temperature |
|
DSM Akulon® F132-E1 PA6
Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion
|
|||
| Processing Temperature | 270 °C | 518 °F | Extruder Temperature |
|
DSM Akulon® F136 PA6
Very High Viscosity, Film Extrusion
|
|||
| Processing Temperature | 270 °C | 518 °F | Extruder Temperature, film |
|
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR15 NL HS PA6.6, 15% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
|
E-Polymers TEKAMID® TA250GFR , Flame Retardant, 25% Glass Fiber Reinforced PA66, DAM
GF reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
|
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM
40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
E-Polymers TEKAMID® TB120G60W , 62% Glass Fiber Reinforced PA6, DAM
High strength, weather resistanceInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
|
E-Polymers TEKANATE™ G710 , 10% Glass Fiber Reinforced Poly Carbonate
10% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
|
E-Polymers TEKANATE™ G720 , 20% Glass Fiber Reinforced Poly Carbonate
20% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
|
E-Polymers TEKANATE™ G730 , 30% Glass Fiber Reinforced Poly Carbonate
30% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 °C | 518 °F | Extruder Temperature |
|
DSM Akulon® XP32-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 CR10 BK111 PA6.6, 10% carbon fiber reinforced, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
|
Eurotec® Tecopet® PT74 CR30 BK111 PR PET, 30% carbon fiber reinforced, black, fast crystallization grade
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
|
Eurotec® Tecotek® PC40 GR30 NL PC, 30% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
|
Eurotec® Tecotek® PC43 GR30 BK002 PC, 30% glass fiber reinforced, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 °C | 518 °F | Injection, recommended |
|
Arkema Group Rilsan® Clear G380 Renew Polyamide
Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited..
|
|||
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | Resin Temperature |
|
Asahi Kasei Xyron® A1400 PPE/PA
Oil ResistantInformation provided by Asahi Kasei
|
|||
| Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
|
Arkema Group LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. Main applicationsLOTADER 3210 is a versatile adhesive for extrusi..
|
|||
| Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
|
Arkema Group LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3410 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3410 is a versatile adhesive for extrusion coating or lam..
|
|||
| Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
|
Arkema Group LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3430 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3430 is a versatile adhesive for extrusion coating or lam..
|
|||