Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 554 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
See Materials Notes
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry)  (discontinued **)
Capron 5233G is a 33% glass fiber reinforced, polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineerin..
Processing Temperature 290 °C
554 °F
See Materials Notes
BASF Capron® 5233G HS BK-102 33% Glass-Filled Nylon 66 (Dry)  (discontinued **)
Capron 5233G HS BK-102 is a 35% glass reinforced, heat stabilized, pigmented black nylon 6,6 injection molding compound offering excellent strength, rigidity, stiffness, creep resistance, and dimens..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-1114 Polyamide 66, with carbon fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-7332/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-7395 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-8064 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-8181 Polyamide 66, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 8-7190 High impact polyamide, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1/GF/20/TF/10/SI/2/NC Polyamide 66, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/BK Polyamide 66, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS/BK Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Improved friction and wear behaviour. Emergency running propert..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-0784 Polyamide 66, with glass fiber and carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-1119-1 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-7360/EG Polyamide 66, with PTFE, lubricant modified, high viscosity, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property.Bea..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-7701 Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-7893/GY Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-7956 Polyamide 66, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Processing Temperature <= 290 °C
<= 554 °F
Kingfa JH710 G20 Flame Retardant & 20% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® GS-H/2 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele..
Processing Temperature 290 °C
554 °F
Shinil Chemical SHINCON PPS-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Processing Temperature <= 290 °C
<= 554 °F
DuPont™ Fusabond® E158H Polymer Modifier
DuPont™ Fusabond® E158H is a anhydride modified polyethylene. Uses: Adhesives Coating Applications Pipe Coating Tie-Layer
Processing Temperature 290 °C
554 °F
Approximate middle barrel temperature.
A. Schulman ComAlloy Comtuf® 635 Nylon 6/6, Glass/Mineral Reinforced, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has ..
Processing Temperature 290 °C
554 °F
Approximate middle barrel temperature.
A. Schulman ComAlloy Hiloy® 636 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Processing Temperature 290 °C
554 °F
Approximate middle barrel temperature.
A. Schulman ComAlloy Hiloy® 657 Nylon 6/6, Carbon/Glass Fiber Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Processing Temperature 290 °C
554 °F
Approximate middle barrel temperature.
A. Schulman ComAlloy Lubrilon® 635 Nylon 6/6, Carbon Fiber/PTFE Filled, Proprietary Lubricant Package
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Processing Temperature 290 °C
554 °F
See Materials Notes
BASF Capron® 5202CQ Blend HS Blend Nylon 66 (Dry) &nbsp;(discontinued **)
Capron 5202CQ HS Blend is a heat stabilized, blended polyamide 6,6 injection molding homopolymer developed for fast molding cycles. It is also available in pigmented versions.Capron 5202CQ HS Blend..
Processing Temperature <= 290 °C
<= 554 °F
DuPont™ Fusabond® E226 Polymer Modifier
DuPont™ Fusabond® E226 is a anhydride modified polyethylene. Uses: Wire & Cable Applications Polymer Modifier Fusabond E226 resin conforms with the Code of Federal Regulations, Title 21, Paragra..
Processing Temperature 290 °C
554 °F
mass temp
Lehmann & Voss LUVOCOM® 1-7497 Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Copyright © lookpolymers.com All Rights Reserved