| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 289 °C Grade Count:31 |
|
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 284 °C Grade Count:7 |
|
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 284 °C Grade Count:5 |
|
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR25 NL HS PA6.6, 25% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR30 NL HS PA6.6, 30% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR30 NL RM PA6.6, 30% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR40 NL HS PA6.6, 40% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 MF40 BK001 HS PA6.6, 40% mineral filled, heat stabilized, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
|
E-Polymers TEKAMID® TA210GM , GF/MF Reinforced PA66, DAM
GF/MF reinforced, Heat resistance, Low warpageInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
|
E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM
40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
|
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM
15% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
|
E-Polymers TEKAMID® TA250GM , GF/MF Reinforced PA66, DAM
GF/MF reinforced, Good surface, Low warpageInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 CR10 BK111 PA6.6, 10% carbon fiber reinforced, black
Information provided by Eurotec®
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
|
E-Polymers TEKAMID® TA210G33 , 33% Glass Fiber Reinforced PA66, DAM
33% Glass Fiber reinforced, High strengthInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
|
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET
45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae..
|
|||
| Processing Temperature | 250 - 300 °C | 482 - 572 °F | Resin Temperature |
|
Asahi Kasei Xyron® X0722 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
|
|||
| Processing Temperature | 285 - 300 °C | 545 - 572 °F | Melt |
|
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
|
|||
| Processing Temperature | 250 - 300 °C | 482 - 572 °F | Injection |
|
Arkema Group Rilsan® Clear G350 Polyamide
Rilsan® Clear G350 is a high performance transparent polyamide. This grade has been specially designed for injection molding applications, ideally suited for optics as high end eyewear frames.Infor..
|
|||
| Processing Temperature | 170 - 300 °C | 338 - 572 °F | |
|
Asahi Kasei ASACLEAN HP Polypropylene Based Purging Compound
HP was developed for Polypropylene color changes for large parts and hot runner cleaning. Its higher melt flow makes HP Grade suitable for high cavitation hot runner cleaning. HP Grade is moldable a..
|
|||
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 287 °C Grade Count:34 |
|
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Processing Temperature | 230 - 300 °C | 446 - 572 °F | |
|
E-Polymers Tekaloy® G70GFR , Flame Retardant, 30% Glass Fiber Reinforced PC/ABS Alloy
30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
|
|||
| Processing Temperature | 240 - 300 °C | 464 - 572 °F | Resin Temperature |
|
Asahi Kasei Xyron® 740V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
|
|||
| Processing Temperature | 110 - 300 °C | 230 - 572 °F | Average value: 237 °C Grade Count:5 |
|
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
|
|||
| Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
|
E-Polymers TEKAMID® TA210G15 , 15% Glass Fiber Reinforced PA66, DAM
Beautiful surface, strength propertyInformation provided by E-Polymers Co. Ltd.
|
|||