| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
|
Northstar Polymers MGB-A80AQ High Performance Polyurethane Cast Elastomer System 80A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
|
|||
| Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
|
Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
|
|||
| Processing Temperature | 82.2 °C | 180 °F | Prepolymer Temperature |
|
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer
This two-component polyurethane casting system makes type of soft elastomer material known as “gel”. Applications for this material include filling component for computer keyboard/mouse-pad wrist..
|
|||
| Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
|
Northstar Polymers MSB-A95A High Performance Polyurethane Cast Elastomer System
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
|
|||
| Processing Temperature | 82.2 °C | 180 °F | Prepolymer Temperature |
|
Northstar Polymers MSS-A70GQ High Performance Polyurethane Cast Elastomer System 70A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires cut/tear resistance, dry-abrasion resistance, slow resp..
|
|||
| Processing Temperature | 82.2 °C | 180 °F | Curing Agent Temperature |
|
Northstar Polymers MSS-A70GQ High Performance Polyurethane Cast Elastomer System 70A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires cut/tear resistance, dry-abrasion resistance, slow resp..
|
|||
| Processing Temperature | 82.2 °C | 180 °F | Curing Agent Temperature |
|
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
|
|||
| Processing Temperature | 82.2 °C | 180 °F | Curing Agent Temperature |
|
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
|
|||
| Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
|
Northstar Polymers MSS-A85C Ester Base Polyurethane
This high performance polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhibit hig..
|
|||
| Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
|
Northstar Polymers MSS-A90A High Performance Polyurethane Cast Elastomer System 90A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
|
|||
| Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
|
Northstar Polymers MSS-A95BQ Ester Base High Performance Polyurethane
This high-performance quasi-polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhib..
|
|||
| Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Curing Agent Temperature |
|
Northstar Polymers MSS-A95BQ Ester Base High Performance Polyurethane
This high-performance quasi-polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhib..
|
|||
| Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
|
Northstar Polymers MGG-A70DQ High Performance Polyurethane Cast Elastomer System 70A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
|
|||
| Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
|
Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contac..
|
|||
| Processing Temperature | 82.2 °C | 180 °F | Mold and Set Temperature |
|
Spartech Polypedic A Low Density Polyethylene
Description: Flexible, lower processing temperature, softApplications: Anterior shells for AFOs and KAFOs; TLSOs; passive types of HOs, WHOs and EWHOsInformation provided by Spartech.
|
|||
| Processing Temperature | 82.2 °C | 180 °F | Mold and Set Temperature |
|
Spartech Polypedic F High Density Polyethylene
Description: More rigid, tough, able to withstand cold temperature applicationApplications: Neck brace; splintsInformation provided by Spartech.
|
|||
| Processing Temperature | 82.2 °C | 180 °F | Mold and Set Temperature |
|
Spartech Polypedic Modified Low Density Polyethylene
Description: Flexible, wider window for forming, softApplications: Anterior shells for AFOs and KAFOs; TLSOs; passive types of HOs, WHOs and EWHOs; prosthetic flexible socketsInformation provided by..
|
|||