Processing Properties Metric English Comments
Injection Pressure 50.0 - 80.0 MPa
7250 - 11600 psi
Plastcom SLOVALEN PC 78 FRD 3 Polypropylene Copolymer, Halogen Flame Retardant
FeaturesDetermined for environment where contact with water is possible because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machine..
Injection Pressure 50.0 - 80.0 MPa
7250 - 11600 psi
Plastcom SLOVALEN PC 88 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized
FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with..
Injection Pressure 50.0 - 80.0 MPa
7250 - 11600 psi
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant
FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5300 is a static dissipative thermoplastic compound based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance valu..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound
PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..
Injection Pressure 40.0 - 80.0 MPa
5800 - 11600 psi
Polykemi AB POLYelast TPE 10012 R3 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PE 1292
PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound
PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PE 1299 Conductive Thermoplastic Compound
PRE-ELEC® PE 1299 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1299 has a high concentration o..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PP 1378
PRE-ELEC PP 1378 is a conductive thermoplastic compound based on glass-fiber reinforced polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electri..
Injection Pressure 40.0 - 80.0 MPa
5800 - 11600 psi
Polykemi AB POLYelast TPE HJ-75 UV1 Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE
Information provided by Polykemi AB
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PP 1383
PRE-ELEC PP 1383 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Injection Pressure 40.0 - 80.0 MPa
5800 - 11600 psi
Polykemi AB POLYelast TPE HJ753 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PP 1385
PRE-ELEC PP 1385 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PP 1392 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PP 1392 is a carbon black filled conductive thermoplastic compound based on polypropylene. In addition to a low electrical resistivity PRE-ELEC® PP 1392 has an excellent balance of mecha..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound
PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PP 1395
PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resist..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® 12-031  (discontinued **)
PRE-ELEC 12-031 is a conductive thermoplastic compound based on a polyacetal copolymer with 10% carbon fiber. PRE-ELEC 12-031 exhibits excellent mechanical properties and electrical conductivity. Te..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® 12-032  (discontinued **)
PRE-ELEC 12-032 is a conductive thermoplastic compound based on a polyacetal copolymer with 20% carbon fiber. PRE-ELEC 12-032 exhibits excellent mechanical properties and electrical conductivity. Te..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® 12-033  (discontinued **)
PRE-ELEC 12-033 is a conductive thermoplastic compound based on a polyacetal copolymer with 30% carbon fiber. PRE-ELEC 12-033 exhibits excellent mechanical properties and electrical conductivity. Te..
Injection Pressure 40.0 - 80.0 MPa
5800 - 11600 psi
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 50.0 - 80.0 MPa
7250 - 11600 psi
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads
PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PA 1409 Conductive Thermoplastic Compound
PRE-ELEC® PA 1409 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound
PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P..
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PA 1408 Conductive Thermoplastic Compound
PRE-ELEC® PA 1408 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..