| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
|
Lubrizol Estane® S395A Thermoplastic Polyurethane
Type: Estane® S395A is a Shore 95A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availa..
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
|
Lubrizol Estane® S398A Thermoplastic Polyurethane
Type: Estane® S398A is a Shore 98A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi..
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant CA9000NAT` Acetal Copolymer
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant PA612G30 Nylon 612, 30% Glass Fiber, Impact Modified
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol 60G13HSP Black Nylon 6, 13% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol ABS5475 ABS, General Purpose, Low Gloss
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol BR7008 Polycarbonate/Polyester Alloy
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol BR7039 Nylon 6 Alloy, bondable to TPU
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA113C Nylon 66, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA113G15 Nylon 66, 15% Glass Fiber
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA1SP0003 Nylon 66, PE Modified
Reduced Coefficient of FrictionData provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA211 Nylon 6, General Purpose
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA211G13 Nylon 6, 13% Glass Fiber
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA211G50 Nylon 6, 50% Glass Fiber, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA213G30 Nylon 6, 30% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA233G13 Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Toughened
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA2SP0003 Nylon 6, High Gloss
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA2SP0008HW Nylon 6, Heavyweight Compound
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA2SP0017 Nylon 6, Impact Modified
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA2SP0022 Nylon 6, Impact and Flow Modified, ESD Protection, Black
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant PA223 Nylon 6, Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol 6004G23 Nylon 6, 23% Glass Fiber Reinforced
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
|
Clariant Renol 66G33-L Nylon 66, 33% Glass Fiber Reinforced, Lubricated
Data provided by Clariant Masterbatches
|
|||