| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
|
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
|
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
|
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
|
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.41 - 8.27 MPa | 350 - 1200 psi | |
|
Multibase Nylex™ 2185 FR Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric..
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant ABS4500 ABS, High Impact
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant CA9000NAT` Acetal Copolymer
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant PA123G30 Nylon 66, 30% Glass Fiber, Impact Modified, Heat Stabilized
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant PA213M40 Nylon 6, 40% Mineral Reinforced, Heat Stabilized
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol 66G33 2% Moly Nylon 66, 33% Glass Fiber Reinforced, 2% Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol ABS3460 ABS, General Purpose, Low Gloss
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol BR4014BK ABS, High Gloss, Black
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PA111G35IF Nylon 66, 35% Glass Fiber, Improved Flow
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PA111G50IF Nylon 66, 50% Glass Fiber, Improved Flow
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PA211G40 Nylon 6, 40% Glass Fiber, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PA213G30 Nylon 6, 30% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PA2SP0024 Nylon 6, Flame Retardant, Static Dissipative
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PCSP0006 Polycarbonate, Laser Markable
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
|
Clariant Renol POMSP0001 Acetal Copolymer, Aramid Fiber, PTFE Lubricated
Data provided by Clariant Masterbatches
|
|||