| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | |
|
Plastcom PLASTAMID® 6 GF 20 002 PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 20% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, ..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | |
|
Plastcom PLASTAMID® 6 GF 25 002 PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 25% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, ..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | |
|
Plastcom PLASTAMID® 6 GF 30 005 PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 30% glass fiber, used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 CFHI Polyamide 6 - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 GF15 I Polyamide 6 - Glass Fiber Reinforced
15% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 MCS I8 Polyamide 6 - Impact Modified
Increased impact resistance grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main propert..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural
Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.For ..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural
Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | injection speed: 80 - 120 rpm |
|
Beijing Chemical Industry KAIFA® GL1200 ABS General Purpose Grade
Middle impact, Good mechanical strength, High flexural strengthInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | injection speed: 80 - 120 rpm |
|
Beijing Chemical Industry KAIFA® GL2100 ABS Good Flow Grade
Good flow, Easy processing, High glossInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | injection speed: 80 - 120 rpm |
|
Beijing Chemical Industry KAIFA® GL2200 ABS Good Flow Grade
High impact, Easy processingInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | injection speed: 80 - 120 rpm |
|
Beijing Chemical Industry KAIFA® GL3200 ABS Flame-Retardant Grade
Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced
20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following ..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV2 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, flammability class V2, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning...
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced
Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has ..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 MCS HI Polyamide 6 - Impact Modified
Very high impact resistance, cold impact grade (to -40°C). Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has t..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 MHLS Polyamide 6 - Colored
Heat and UV light stabilized grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main proper..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 MT30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored
Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | injection speed: 80 - 120 rpm |
|
Beijing Chemical Industry KAIFA® GL1300 ABS General Purpose Grade
Excellent impact properties at low temperaturesInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | injection speed: 80 - 120 rpm |
|
Beijing Chemical Industry KAIFA® GL3100 ABS Flame-Retardant Grade
Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | injection speed: 80 - 120 rpm |
|
Beijing Chemical Industry KAIFA® GL5100 ABS Extrusion Grade
Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
|
|||
| Injection Pressure | 80.0 - 130 MPa | 11600 - 18900 psi | 80 MPa is recommended |
|
Azoty Tarnow™ Tarnamid® T-27 GF25 M Polyamide 6 - Improved Slip Properties
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid..
|
|||
| Injection Pressure | 70.0 - 130 MPa | 10200 - 18900 psi | |
|
Suzhou Hipro Polymers Hiprolon® 90 MC HLS G30 Nylon 612, 30% glass fiber filled
Hiprolon® 90 MC HLS G30 is a polyamide 6.12 compound reinforced with 30% chopped glass fiber, and is used for injection molding. Features: high dimension stability, chemical resistance, impact resi..
|
|||