| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
|
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66
Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a..
|
|||
| Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
|
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6
Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo..
|
|||
| Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
|
Plastcom SLOVASTER® B GB 30 PBT, 30% glass beads
FeaturesPBT for injection moulding, chemically reinforced with 30% glass beads. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
|
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66
Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
|
|||
| Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
|
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Injection Pressure |
30.0
-
100
MPa <br>@Time 2.00 - 10.0 sec
|
4350
-
14500
psi <br>@Time 0.000556 - 0.00278 hour
|
|
|
Gromax 1163LL TPE
163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext..
|
|||
| Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
|
Gromax CCP PBT 1100-220S
Product Description: PBT unreinforced and impact-modified injection molding grade. Characteristics:Low warp age, high toughness and excellent dimensional stabilityExcellent glossy surface and less-g..
|
|||
| Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
|
Gromax PBT 1100-211S
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Injection Pressure | 40.0 - 100 MPa | 5800 - 14500 psi | 3-15 sec |
|
Zhejiang Juner 301-G0 Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
|
|||